The GMAW torch orientation, whether pulling or pushing, influences both arc welding and hybrid processes. In hybrid laser-arc welding, for example, when the torch is pulled, a greater bead penetration is obtained. To promote greater penetration, the literature also indicates the use of a buried arc in GMAW, although it was initially developed to only operate with a vertically-positioned torch. Therefore, this work aims to investigate the influence of the push and pull techniques on the behavior of buried-arc GMAW at high welding speeds. Welds were performed with the push and pull techniques under the following conditions: buried and unburied (long) arc with welding speeds of 1.0, 1.5 and 2.0 m/min and current ranging from 450 to 470 A. The process tends to be more stable when pulling than when pushing (buried or long arc). Evidence of instability was only identified for the pushed buried arc, due to material accumulation at the front region of the molten pool, for the higher welding speeds. Only the 1.0 m/min buried-arc processes resulted in beads with an appropriate surface finish.
Nanotechnology is the domain of technological development and application of materials which go from 1 to 100 nm in at least one of their dimensions. The use of nanoparticles in engineering focuses on the development of new materials with special properties, which can be used as filler materials in the welding field. In this context, this study contributes to the stage preceding the deposition of the weld beads. This work aims to insert, using the colloidal processing technique, ceramic nanoparticles (ZrO2) into a Co-based superalloy (Stellite 6) and study the solidification of this "nanocomposite". 4 filler materials in the shape of compacted cylinders were melted by PTA: Stellite 6 with added Fe carriers with ceramic nanoparticles (ZrO2) (1%, 2.5% and 7.5% volume) and Stellite 6 without any additions. The molten materials were characterized through optical and scanning electron microscopy with field emission (SEM-FEG), XRD and Vickers microhardness. The results show that the colloidal processing technique was effective in adhering the ZrO2 nanoparticles to the carrier Fe particles, which were mixed with Stellite 6, as well as the relationship between microstructure refinement, phases and microhardness after PTA melting.
The design of casting components is a complex activity, which is usually based on guidelines scattered in the literature, or based on the designer’s accumulated experience. A single failure in the casting process selection can increase design and production time and, in critical cases, result in a collapse of the manufacturing and assembly of components. Nowadays the selection is made by prioritizing the features of the casting process, but this action could be carried out during the product development stage, assisting the designer. This could allow the project to adjust to a more viable casting process. In this context, our goal is to propose a selector for casting processes to be used during the early stages of the embodiment design. It was achieved through the use of quality function deployment and design for manufacturing (DFM) principles. Our proposal relates the component’s main functions with each process characteristic (mass, minimum section thickness, draft angle, surface finish, dimensional tolerances, minimum lot and lead time) through a correlation matrix, resulting in importance indexes for these characteristics. Furthermore, the importance indices obtained are related to the capability of each casting process discussed, providing a process rating. A checklist based on DFM principles is also provided to guide the designer when a need for improvement is observed or no processes are suited for producing the desired part. For validation, two ferrous and two nonferrous cast parts were analyzed. The results were compared with other selectors described in the literature and with processes actually used in the industry. Thus, they have shown a good relation with the other methods, especially regarding the quantitative classification determined by the proposed selector.
>Injection molds can fail after a certain period of use, which may compromise the final part’s integrity and quality, but that can be solved using welding repair processes. This work aimed to investigate the influence of AISI P20 molds repaired by Gas Tungsten Arc Welding (GTAW) and Nd-YAG laser-welding processes on the properties of injection-molded parts with semi-crystalline (polypropylene) and amorphous (polycarbonate and acrylonitrile butadiene and styrene terpolymer) thermoplastics. Welds were prepared by machining 0.8 mm-deep 40 mm x 5 mm grooves to be filled by GTAW and Nd-YAG laser-welding deposits, in order to simulate the repair of AISI P20 molds. All polymers were injected into weld-repaired and unrepaired molds, and then evaluated in terms of microstructure, crystallinity degree, mechanical properties and gloss. The results suggest that the repaired region for both studied welding processes, despite the difference in hardness of the weld region, does not significantly affect the properties of semi-crystalline and amorphous injected polymers.