Densely consolidated WC-based hard materials with 5–20 vol% ZrSiO4 was fabricated by spark plasma sintering at 1400 ℃ at a constant heating rate of 70 ℃/min−1. To achieve mechanical alloying of WC-ZrSiO4, planetary ball milling was carried out for 12 h, during which the brittle-brittle components (WC-ZrSiO4) became fragmented and their particles became refined. It was observed that certain, specific, non-isothermal sintering kinetics, such as apparent activation energy, sintering exponents, and densification strain, affected the densification behavior. The evolution of phase structure from powder to compact was found to be related the lattice distortion and micro-strain in the basal planes of WC. By examining the mechanical properties of the samples, it was that the added zircon content leads to enhanced fracture toughness (12.9 MPa m1/2) owing to the presence of WC-ZrSiO4 in the cemented carbide. In fact, the microcrack propagation of the fracture passed through zircon from a transgranular to a ductile component (fcc) where the crack tips could be absorbed. Graphic
5 August 2020 in Korean Journal of Metals and Materials
In this study, consolidated WC-Fe compacts as a function of Fe contents were fabricated by a spark plasma sintering method, following the mixed by the ball-milled powder. Fe among the metallic binders was added to WC enhance not only the driving force of sintering process but also suppressing the grain growth. WC-Fe mixed powder samples were fabricated with 5, 10 and 15 wt.% Fe contents, and the particle sizes of the mixed powders were determined to be 2.15 to 3.15 µm, respectively. The WC-Fe mixed powders were processed by spark plasma sintering, at a sintering temperature of 1300 oC. Consequently, the relative densities of the WC-5, 10 and 15 wt.% Fe sintered-bodies were about 99.2, 99.5 and 100%, respectively. The grain sizes of the WC-5, 10 and 15 wt.% Fe sintered-bodies were about 0.92, 0.98 and 1.02 µm, respectively. The Fe particles penetrated into the WC particles by dissolving and re-precipitation, and the final sintered bodies were completely densified. The mechanical properties of the WC-Fe sintered-bodies exhibited a hardness up to 1934 kg·mm2 and a fracture toughness above 6.88 MPa·m1/2. The microstructure behavior of the WC-Fe sintered-bodies was investigated in terms of mechanical properties to examine their properties for various Fe contents. In addition, the mechanical and physical properties were compared with the reported values for other sintering-processes, i.e. HFIHS, HIP, etc.
1 February 2020 in Metals and Materials International
In this study, Binderless-WC hard materials were fabricated using the pulsed current activated sintering (PCAS) process for a Friction Stir Welding tool and difficult-to-cut tool application. Tungsten carbide (WC) hard materials are used in various industries and possess a superior hardness compared to other hard materials. They have particularly high melting points, high strength, and abrasion resistance. 100 mm diameter and 5 mm thick binderless-WC hard materials were fabricated using a 30,000 A pulsed current activated sintering machine and 0.3 to 0.5 µm size WC powders. Variation of properties in binderless WC hard materials by sintering temperature were increased slightly for 0.11 to 0.37 um with a grain size and densified completely for 70.0 to 99.5% for a relative density. Consequently, these materials were almost completely dense with a relative density of up to 99.5% after simultaneous application of 60 MPa pressure and an electric current for 2 min at 1600 o C, almost without any significant change in the crystallite size. The average WC crystallite size that was produced through PCAS was 0.37 µm at 1,600 °C. In terms of mechanical properties, considering only the densified sintered body that the hardness and fracture toughness of binderless-WC hard materials were about 2,661.5 kg/mm 2 and 3.90 MPa•m 1/2 , respectively.