The environmental problem generated by the massive consumption of plastics makes necessary the developing of biodegradable antimicrobial materials that can extend food shelf-life without having a negative impact on the environment. The current situation regarding the availability of biodegradable food packaging materials has been analysed, as well as different studies where antimicrobial compounds have been incorporated into the polymer matrix to control the growth of pathogenic or spoilage bacteria. Thus, the antimicrobial activity of active films based on different biodegradable polymers and antimicrobial compounds has been discussed. Likewise, relevant information on biodegradation studies carried out with different biopolymers in different environments (compost, soil, aquatic), and the effect of some antimicrobials on this behavior, are reviewed. In most of the studies, no relevant effect of the incorporated antimicrobials on the degradation of the polymer were observed, but some antimicrobials can delay the process. The changes in biodegradation pattern due to the presence of the antimicrobial are attributed to its influence on the microorganism population responsible for the process. More studies are required to know the specific influence of the antimicrobial compounds on the biodegradation behavior of polymers in different environments. No studies have been carried out or marine media to this end.
Starch (S) films containing gellan gum (90:10) and polyester (P) blend films (PLA:PHBV, 75:25) with and without ferulic, p-coumaric or protocatechuic acid at 2% (w/w) were obtained by melt-blending and compression moulding for the purposes of obtaining SP bilayers by thermo-compressing both monolayers together. These were characterised as to their mechanical and barrier properties and as to their performance as packaging materials for pork meat slices. The incorporation of phenolic acids promoted the water vapour and oxygen barrier capacity of bilayers while reducing their stiffness and resistance to break, mainly in the case of protocatechuic acid. Phenolic acids significantly improved the antioxidant capacity of the bilayer films, reducing the lipid oxidation of packaged meat during storage. Phenolic acid loaded bilayers also reduced the microbial counts of meat, mainly for lactic acid bacteria. These effects positively affected the development of the sample pH and colour parameters throughout storage. Active starch-polyester bilayer films exhibited great potential as a means of extending the shelf-life and improving the quality preservation of pork meat.
In the present study, the effectiveness of a multilayer film of polylactide (PLA), fully bio-based and compostable, was ascertained to develop a novel sustainable packaging solution for the preservation of fresh pork meat. To this end, the multilayer PLA films were first characterized in terms of their thermal characteristics, structure, mechanical performance, permeance to water and aroma vapors and oxygen, and optical properties and, for the first time, compared with two commercial high-barrier multilayer packaging films. Thereafter, the multilayers were thermosealed to package fillets of fresh pork meat and the physicochemical changes, lipid oxidation levels, and microbiological counts were monitored in the food samples during storage under refrigeration conditions. Results showed that the meat fillets packaged in PLA developed a redder color and showed certain indications of dehydration and oxidation, being more noticeably after 11 days of storage, due to the higher water vapor and oxygen permeance values of the biopolymer multilayer. However, the pH changes and bacterial growth in the cold-stored fresh pork meat samples were minimal and very similar in the three tested multilayer films, successfully accomplishing the requirements of the food quality and safety standards at the end of storage.
Bilayer films of cassava starch-based (with 10% gellan gum) and polylactic (PLA): Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) polyester blend (with 75% PLA) monolayers were obtained by melt-blending and compression-molding, and the subsequent thermocompressing of both monolayers. Ferulic acid (FA) was incorporated into the polyester sheet by spraying and drying. Films were characterized in terms of their microstructure and functional properties throughout two months of storage at 25 °C and 53% relative humidity. The laminates exhibited improved tensile and barrier properties compared to the respective monolayers, which makes them more adequate for food packaging purposes. Surface incorporation of ferulic acid did not significantly modify the barrier and mechanical properties of the films while providing them with antioxidant and antibacterial capacity when applied in aqueous systems, where a complete release of active compounds occurred. The physical properties of the bilayers and layer thermo-sealing were stable throughout storage. Likewise, the antioxidant and antimicrobial active properties were preserved throughout storage. Therefore, these active bilayers represent a sustainable packaging alternative to non-biodegradable, non-recyclable synthetic laminates for food packaging purposes, which could extend the shelf-life of food due to their antioxidant and antibacterial properties.
Films based on a 75:25 polylactic acid (PLA) and Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) blend, containing 2% (w/w) of different phenolic acids (ferulic, p-coumaric or protocatechuic acid), and plasticised with 15 wt. % polyethylene glycol (PEG 1000), were obtained by melt blending and compression moulding. The disintegration and biodegradation of the film under thermophilic composting conditions was studied throughout 35 and 45 days, respectively, in order to analyse the effect of the incorporation of the antimicrobial phenolic acids into the films. Sample mass loss, thermo-degradation behaviour and visual appearance were analysed at different times of the composting period. No effect of phenolic acids was observed on the film disintegration pattern, and the films were completely disintegrated at the end of the composting period. The biodegradation analysis through the CO2 measurements revealed that PLA-PHBV blend films without phenolic acids, and with ferulic acid, completely biodegraded after 20 composting days, while p-coumaric and protocatechuic slightly retarded full biodegradation (21 and 26 days, respectively). Phenolic acids mainly extended the induction period, especially protocatechuic acid. PLA-PHBV blend films with potential antimicrobial activity could be used to preserve fresh foodstuff susceptible to microbial spoilage, with their biodegradation under composting conditions being ensured.
This work reports on the development and performance evaluation of newly developed paper sheets coated, on both sides, with thin films of biodegradable poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) for applications of food packaging. For this, PHBV/paper/PHBV multilayers were first prepared by the thermo-sealing technique, optimizing the process variables of temperature and time. Thereafter, the multilayer sheets were characterized in terms of their morphological, optical, thermal, mechanical, and barrier properties and compared with equivalent paper structures double coated with high-barrier multilayer films of petrochemical polymers. The results indicated that the double coatings of PHBV successfully improved the mechanical resistance and ductility, protected from moisture, and also reduced the aroma and oxygen permeances of paper, having a minimal effect on its optical and thermal properties. Finally, the compostability of the resultant multilayer sheets was analyzed, confirming that the presence of the PHBV coatings slightly delayed the aerobic biodegradation and disintegration of paper.