MoS2 is a very popular solid lubricant that has significant applications in the field of aerospace and automobiles. Due to its affinity towards oxygen and moisture, it has been modified through different mechanisms, such as doping and co-doping. This review comprehensively analyzes advanced materials used to alter MoS2, highlighting their impact on wear resistance, mechanical durability, and environmental stability. Additionally, we discuss the latest fabrication and synthesis techniques tailored for tribological applications, emphasizing their role in improving coating performance. By elucidating the mechanisms through which dopants contribute to multifunctional MoS2 coatings, this review offers valuable insights into their potential for next-generation lubrication technologies. The findings presented here serve as a foundation for future research to optimize MoS2-based coatings for extreme environments and multifunctional applications. Graphical Abstract
The poor tribological and mechanical performance of Al alloys hinders their use in practical applications where low COF and high durability are required. This study examined and evaluated a novel laser-sintered Ni-Cr coating to improve the load-carrying capacity and tribological performance of an Al alloy (Al 6061) substrate. The authors demonstrate that laser sintering cycle count is a decisive process variable governing coating dispersion, microstructural consolidation, and tribological performance in Ni-Cr coatings fabricated via Selective Laser Sintering (SLS). Increasing the laser cycle count progressively refined the surface morphology, improved coating dispersion, and strengthened interparticle bonding. As a result, the average durability after three cycles was seven times that after one laser cycle, accompanied by markedly improved COF. To further improve durability and load-carrying capacity, Ti3SiC2 was introduced into the Ni-Cr coating. The coating containing 10 wt% Ti3SiC2 exhibited a 20-fold increase in durability, extending the time to failure to approximately 70,000 s (700 m) while maintaining a low coefficient of friction (~0.48) compared with the coating containing no Ti3SiC2. The greater durability of the Ni-Cr-10wt%Ti3SiC2 coating in this novel study was attributed to improved adhesion to the substrate, better particle distribution during sintering, and greater load-carrying capacity. While further process changes do not yield feasible samples, this study showed that surface properties can be improved within the available small-process regime. Overall, laser sintering of a Ni-Cr-10wt%Ti3SiC2 coating shows promise as a means to improve the tribological and mechanical performance of Al 6061. This study should aid researchers and other stakeholders in fabricating well-adhering, durable, and tribotactic composite coatings on Al6061 and similar material systems.