1 September 2022 in Materials
Verified
Journal Article
Open access
PDF file
SLSheng Li
Sheng Li
HLHongbo Li
Hongbo Li
CYChangyu Yan
Changyu Yan
YDYongfa Ding
Yongfa Ding
XZXuanshuo Zhang
Xuanshuo Zhang
JZJing Zhao
Jing Zhao
Although fly ash foam concrete (FAFC) is lightweight, heat-retaining, and insulating, its application options are constrained by its weak construction and short lifespan. The effects of various dosage ratios of the foaming agent (i.e., hydrogen peroxide), silica fume, and polypropylene fiber on the dry density, compressive strength, thermal insulation performance, pore structure parameters, and durability of FAFC were analyzed in this study, which sought to address the issues of low strength and low durability of FAFC. According to the findings, there is a negative correlation between the amount of hydrogen peroxide (as the foaming agent) and compressive strength, and, as the silica fume and polypropylene fiber (PP fiber) content rise, the strength will initially rise and then fall. The distribution of pore sizes gradually shifts from being dominated by small pores to large pores as the amount of foaming agent increases, while the porosity and average pore size gradually decrease. When the hydrogen peroxide content is 5%, the pore shape factor is at its lowest. The pore size distribution was first dominated by a small pore size and thereafter by a large pore size when the silica fume and PP fiber concentration increased. Prior to increasing, the porosity, average pore size, and pore shape factor all decreased. Additionally, the impact of PP fiber on the freeze–thaw damage to FAFC was also investigated at the same time. The findings indicate that the freeze–thaw failure of FAFC is essentially frost heave failure of the pore wall. The use of PP fiber is crucial for enhancing FAFC’s ability to withstand frost. The best frost resistance is achieved at 0.4% PP fiber content. In conclusion, the ideal ratio for overall performance was found to be 5% hydrogen peroxide content, 4% silica fume content, and 0.1% polypropylene fiber content. The results obtained could be applied in different fields, such as construction and sustainable materials, among others.

8 December 2021 in Materials
Verified
Journal Article
Open access
PDF file
HLHongbo Li
Hongbo Li
YTYufei Tong
Yufei Tong
HZHubiao Zhang
Hubiao Zhang
XZXuanshuo Zhang
Xuanshuo Zhang
JDJunku Duan
Junku Duan
In order to promote the application of steel slag in road engineering, improve its utilization rate and solve the environmental problems caused by its large accumulation, unconfined compressive strength (UCS) test, indirect tensile strength (ITS) test, freeze-thaw cycle test, dry shrinkage and temperature shrinkage test tests with different steel slag contents were carried out. And the strength formation mechanism of steel slag in base material was revealed by SEM. The results show that the strength of the mixture initially increased and then decreased with increasing steel slag content. The frost resistance increased with increasing steel slag content, which should be limited to no more than 75%. Increasing the steel slag content improved the drying shrinkage resistance but was not conducive to the temperature shrinkage resistance. Microscopic analysis shows that adding a suitable amount of steel slag generated a gel material that was distributed inside the pores. This increased the density of the hardened slurry structure, which improved the strength. The research can provide scientific basis for the application and promotion of steel slag in road base.

25 April 2022 in Materials
Verified
Journal Article
Open access
PDF file
XZXuanshuo Zhang
Xuanshuo Zhang
HLHongbo Li
Hongbo Li
SLSheng Li
Sheng Li
YDYongfa Ding
Yongfa Ding
HZHubiao Zhang
Hubiao Zhang
SHShudong Hua
Shudong Hua
In this study, the silica fume replacement rate, fly ash replacement rate, and curing temperature were regarded as the independent variables, and the compressive and flexural strengths were regarded as the response values. The response surface method was used to construct the response surface polynomial regression model and obtain the optimal preparation parameters of a steel slag cement-based gel slurry (SCGS). The univariate and multivariate effects on the SCGS’s strength were investigated via analysis of variance and a three-dimensional surface model, and the hydration products and strength development law were characterized via scanning electron microscopy and X-ray diffraction. The actual compressive strengths at 3 and 28 d of age were 31.78 and 53.94 MPa, respectively, which were close to the predicted values (32.59 and 55.81 MPa, respectively), demonstrating that the optimized strengths were accurate and reliable. Further, the hydration reaction rate of SiO2 in the silica fume and the physical filling effect of the inert components of fly ash and steel slag under the optimal parameters were the key factors for the early strength of the material. Moreover, continuous C3S hydration in steel slag and the continuous excitation of the volcanic ash properties of fly ash were important factors for the later strength.

20 May 2022 in Materials
Verified
Journal Article
Open access
PDF file
YDYongfa Ding
Yongfa Ding
HLHongbo Li
Hongbo Li
HZHubiao Zhang
Hubiao Zhang
SLSheng Li
Sheng Li
XZXuanshuo Zhang
Xuanshuo Zhang
YTYufei Tong
Yufei Tong
To study the shrinkage and freeze-thaw durability of cement-fly-ash-stabilized brick and concrete reclaimed gravel mixture (CFRBCA), recycled gravel was used to replace 100% of the natural gravel in cement-and-fly-ash-stabilized gravel (CFRCA). Five different mixture ratios of recycled brick and recycled concrete were designed. Dry shrinkage tests, temperature shrinkage tests, freeze-thaw cycle tests, ultrasonic tests, and microscopic analyses were then conducted. The test results showed that the water loss rate, dry shrinkage strain, and dry shrinkage coefficient of CFRBCA increased as the age and brick content increased and tended to be stable by approximately the 40th day of age. The reclaimed gravel content had a great influence on the temperature shrinkage of CFRBCA: the temperature shrinkage coefficient first increased and then decreased as the temperature decreased and reached a peak at −10 to 0 °C. The microstructure analysis showed that as the number of freeze-thaw cycles increases, cracks appear and extend in the CFRBCA, hydration products gradually change from dense to loose, and the Ca/Si ratio increases. Through these experiments, the logarithmic relationship model between ultrasonic wave velocity and CFRBCA strength damage, which can better predict the strength loss caused by CFRBCA variation with freeze-thaw cycles, was established. The brick content is the key parameter affecting the durability of the freeze-thawed CFRBCA, and thus the brick slag content should be properly controlled in engineering applications.

4 October 2023 in Materials
Verified
Journal Article
Open access
PDF file
LSLong Shan
Long Shan
HLHongbo Li
Hongbo Li
JZJing Zhao
Jing Zhao
XZXuanshuo Zhang
Xuanshuo Zhang
KXKang Xinrui
Kang Xinrui
ZZZhiyao Zhou
Zhiyao Zhou
In order to advance the utilization rate of multi-source solid wastes in the Ningxia region of China, 16 groups of pavement base mixtures were designed with cement and fly ash (FA) as binders, steel slag (SS), silicon manganese slag (SMS), and recycled crushed stone (RCS) as composite aggregates. The evolution laws of mechanical and frost resistance properties of the mixture were investigated by unconfined compressive strength (UCS), indirect tensile strength (ITS), freeze–thaw (FT), and ultrasonic detection tests. Then, the strength formation mechanisms were revealed by microscopic characterization technology. The mathematical models between UCS-ITS, UCS-ultrasonic amplitude, FT cycles-UCS damage, and frost resistance coefficient-relative dynamic elastic modulus Er were established. The results show that cement content and curing age exhibited a positive effect on the mechanical strength and frost resistance of the mixture. When the replacement rate of SS was 60%, the mechanical strength and frost resistance were preferable. The R2 of the strength relationship models constructed was greater than 0.9, indicating high fitting accuracy. With the extension of the curing age, the cementitious products such as C-S-H (hydrated calcium silicate) and AFt (ettringite) developed entirely, and they were interlocked and cemented with each other, resulting in the micro-morphology developed from the three-dimensional network structure to the dense system. The macroscopic behavior incarnated that the mechanical strength and frost resistance of the mixture were significantly enhanced.

4 May 2026 in Materials
Verified
Journal Article
Open access
PDF file
JDJunku Duan
Junku Duan
XZXuanshuo Zhang
Xuanshuo Zhang
JZJing Zhao
Jing Zhao
SHShudong Hua
Shudong Hua
HLHongbo Li
Hongbo Li
Silicomanganese slag (SiMnS), a Mn-bearing by-product from silicomanganese alloy production, is often stockpiled in large quantities and may pose environmental concerns due to potential metal leaching. This study develops an OPC-rich hybrid SiMnS–steel slag–fly ash–OPC-activated composite binder, referred to as SMSAB, in which OPC accounts for 55% of the solid precursor mass. Different alkali contents and sodium silicate moduli were investigated, and the optimised paste was characterised in terms of mechanical strength, reaction products, pore structure, carbon-footprint and heavy-metal leaching. The best performance was obtained at an alkali content of 4% and a sodium silicate modulus of 1.0, giving 28-day compressive and flexural strengths of 65.13 MPa and 3.37 MPa, respectively. XRD, SEM-EDS, FTIR and MIP results showed that the main reaction products were C-(A)-S-H, N-A-S-H and C-N-A-S-H gels, which refined the pore structure and produced a dense matrix. The reduction in Mn leaching may be associated with physical encapsulation, possible charge-balancing interactions within gel structures, changes in Mn-related bonding environments and the presence of Mn-bearing phases. Leaching concentrations of Zn, Mn, Cr, Cu and Ni satisfied the Grade III groundwater limits used in China. The calculated carbon intensity of SMSAB was 3.97 kg·(m3·MPa)−1, indicating a favourable strength-to-emission balance compared with the reference systems considered. It should be noted that the present work examines paste specimens only; aggregate skeleton, traffic loading, freeze–thaw cycling and wet–dry/moisture cycling were not included. Therefore, the results demonstrate binder-level potential rather than direct qualification of SMSAB as a pavement base or subbase material.