The presence of defects, grain boundaries and other impurities in Cu2ZnSnS4 (CZTS) thin film material is detrimental on output performances of fabricated solar cells. Moreover the formation of non stable and high resistance contacts to CZTS contribute also to lower the values of short circuit density (Jsc), open circuit voltage (Foc), fill factor (FF) and therefore the efficiency of thin film solar cells. This study evaluates the baseline ZnO/CdS/CZTS cell structure using AMPS-1D program and quantifies reasons for the efficiency limits predicted in such a device. The effect of back contact material, acceptor concentration as well as the absorber thickness on CZTS cell performance is also studied. The solar cell with a back contact work function of 5.6 eV, an acceptor concentration of 4×1015cm-3 and an absorber layer's thickness of 2250 nm showed the best performance with a conversion efficiency of 15.68%. This presented work is essential because it can contribute to fully understand the performance of CZTS solar cell and to fabricate cells with a precise control of the process parameters with a reduced surface as well as bulk recombination and secondary phases.
1 January 1996 in Composites Science and Technology
Metal oxide semiconductor gas sensors are used in a various applications in environmental, industrial and medical field, for instance. They are relatively inexpensive compared to other sensing technologies, robust, lightweight, long lasting and benefit from high material sensitivity and quick response times. Copper oxide (CuO) thin film has been promisingly proposed for chemical sensing applications. Particularly, it has been recommended as a sensitive layer for monitoring harmful and combustible gases. It is an attractive material because of nontoxic, inexpensive, abundance advantages, and its fabrication is easy. In this work, we have synthesized CuO thin films by Spray pyrolysis method. The effect of the temperature deposition is investigated:to say 350 °C, 400 °C, and 450 °C while the deposition duration was kipped to 15 min. The samples were analyzed by X-ray diffraction, Raman spectroscopy, XPS analysis, UV-visible transmission and four points probe method.
CuO thin layers were synthesized using the sol–gel method and deposited onto glass substrates through the dip-coating technique. The impact of annealing temperatures on the structural, optical, and electrical characteristics of the developed CuO thin layers was comprehensively assessed through X-ray diffraction, UV–visible spectrophotometry, and four-point techniques, respectively. X-ray diffraction analysis revealed the formation of CuO thin layers with a distinctive monoclinic tenorite phase structure. The UV–visible spectrophotometer results demonstrated a decrease in transmittance from approximately 30% to about 7% as the annealing temperature increased from 200 °C to 400 °C. The semiconducting properties exhibited temperature-dependent variations, with the band gap narrowing from 1.70 to 1.48 eV as the temperature increased from 200 to 400 °C. Additionally, the electrical conductivity of the CuO layers exhibited a significant increase from 48 to 61 S.m−1 over the same temperature range. Collectively, the findings suggest that an annealing temperature of 400 °C is optimal for achieving well-crystallized CuO layers with desirable characteristics, including high absorbance, low transmittance, a reduced energy band gap, and enhanced electrical conductivity. These results underscore our ability to manipulate CuO properties, offering insights for tailoring them to meet specific requirements, particularly in the context of gas sensor applications.