Poly (ether ether ketone) (PEEK) has attracted increasing attention for dental applications because of its favorable mechanical properties, physicochemical stability, and biocompatibility. However, its inherently poor bonding characteristics remain a major limitation in clinical practice. This study investigated the effect of sequential alumina airborne-particle abrasion (sandblasting) followed by plasma treatment on the bonding performance of methyl methacrylate (MMA)-based luting systems to dental CAD-CAM PEEK. PEEK specimens were prepared as plates and divided into four surface-treatment groups: untreated, airborne-particle abraded, plasma-treated, and airborne-particle abraded followed by plasma treatment. Surface characteristics were evaluated using SEM–EDX analysis and surface roughness measurements, and surface wettability was assessed by contact angle measurements using primers from two MMA-based luting systems (Beautylink [BL] and Super-Bond [SB]). Shear bond strength (SBS) between treated PEEK and each luting system was determined after 24 h of water storage (initial) and after 20,000 thermocycles (aged). Airborne-particle abrasion significantly increased surface roughness, whereas plasma treatment enhanced surface wettability without altering roughness. The combined treatment resulted in the highest surface roughness and the lowest contact angles and demonstrated superior or comparable SBS compared with the single treatments. After aging, the combined treatment significantly improved bonding durability. These findings indicate that airborne-particle abrasion followed by plasma treatment enhances the bonding performance and durability of MMA-based luting systems to PEEK.
This study evaluated the efficacy of bonding of methyl methacrylate -based luting systems to poly(ether ether ketone). Three methyl methacrylate-based systems (Super-Bond [SB], Multibond [MB], and Beautilink [BL]) and an auto-polymerizing poly(methyl methacrylate) resin (Unifast II [UN]) were tested. Tensile bond strength (TBS) was measured before and after thermocycling. Under the initial condition, SB showed significantly higher TBS than BL and UN, whereas no significant difference was observed between SB and MB. After thermocycling, SB exhibited significantly higher TBS than the other groups. Failure mode analysis revealed that SB had fewer adhesive failures than the other groups under both conditions.
1 January 2026 in Asian Pacific Journal of Dentistry
This case report describes a patient with obstructive sleep apnea (OSA) who could not receive oral appliance therapy because of temporomandibular disorders and was instructed to perform tongue rotation exercises. The patient’s maximum tongue pressure, lip-seal strength, and subjective sleep quality improved post-intervention. Furthermore, apnea-hypopnea index and sleep architecture were improved after exercise compared with the baseline. These results suggest that tongue rotation exercises can improve not only oral function but also respiratory function during sleep and, thus, may be meaningful to introduce as an adjunctive therapy for OSA with impaired oral function or intolerance to conventional therapies.
This study evaluated the effects of the methyl methacrylate (MMA)-containing adhesive primer Visio.link on the surface characteristics of sandblasted poly(ether ether ketone) (PEEK) and its bond strength to four dental resin cements: the MMA-based resin cement Super-Bond EX (SB) and the composite-based resin cements RelyX Universal Resin Cement (RX), G-CEM LinkForce (GC), and Panavia V5 (PA). Sandblasted PEEK specimens were tested with or without primer application. Surface morphology, surface roughness, and surface free energy were evaluated, and shear bond strength (SBS) was measured after 1 day of water storage and after 20,000 thermal cycles. Primer application smoothed the sandblasted surface, reduced surface roughness, increased the polar component, and decreased the dispersive component and total surface free energy. Primer application significantly increased the initial SBS of RX, GC, and PA; however, thermal aging reduced bonding durability and caused pretest debonding in several groups. For SB, primer application did not significantly affect the initial SBS, whereas the sandblasted group showed significantly higher SBS than the primer-treated group after aging. The effect of the MMA-containing primer therefore depended on resin cement type and aging condition. These findings suggest that primer application should be considered according to the composition and bonding mechanism of the resin cement rather than routinely incorporated into PEEK bonding procedures.