An attractive method for valorization of glycerol is the catalytic transformation to lactic acid. By overcoming the solubility challenge associated with known homogeneous catalysts for this reaction, we show that thermally robust Ir(I), Ir(III), and Ru(II) N-heterocyclic carbene (NHC) complexes with sulfonate-functionalized wingtips are highly prolific for this process, requiring no cosolvents other than aqueous base. The activity of the catalysts is compared under both conventional heating and microwave conditions. The most active catalyst reaches a TOF of 45 592 h–1 (microwave) and 3477 h–1 (conventional) with 1 equiv of KOH, and proceeds at a constant rate for at least 8 h. Although higher activity is observed with KOH, the catalysts are also highly active with the weaker base, K2CO3 (13 000 h–1 and concurrent formation of formate). The protocol can be modified to achieve quantitative conversion of glycerol in only 3 h. The high activity of these catalysts compared to nonsulfonated analogs is attributed to the stabilization the lactate product in aqueous media. The most active catalyst retains equal activity for crude glycerol. A mechanism is proposed for the most active catalyst precursor involving O–H oxidative addition of glycerol.
15 June 2021 in Environmental Science & Technology
The transfer hydrogenation of CO2 and carbonates from biomass-derived alcohols, such as glycerol, to afford formic and lactic acid is a highly attractive path to valorizing two waste streams, and is significantly more thermodynamically favorable than direct carbonate hydrogenation. Expanding on our seminal report of the first homogeneous catalyst for this process, here we show that thermally-robust and water-soluble Ir(I) and Ir(III) N-heterocyclic carbene (NHC) complexes with sulfonate-functionalized wingtips are highly prolific and robust catalysts for carbonate transfer hydrogenation from glycerol, requiring no additives in aqueous media. The most prolific catalyst of the nine examined, [Ir(NHC-Ph-SO3−)2CO2]Na (cat 7), effectively facilitates the reaction at low catalyst loading (10 ppm) at 150 °C using microwave or conventional heating. The cation of the carbonate salt significantly impacts catalytic activity, with highest activity observed with Cs2CO3 (27 850 and 13 350 TONs for lactate and formate respectively in 6 hours, compared to 15 400 and 8120 with K2CO3). Catalytic amounts of Cs+ were found to significantly enhance activity with K2CO3. Catalyst 7 is even more prolific with conventional heating under a positive N2 pressure, reaching TOFs of >3000 h−1 and >2100 h−1 respectively for lactate and formate with K2CO3. The high activity of this catalyst compared to non-sulfonated and cyclooctadiene analogs is attributed to a combination of catalyst solubility in aqueous media and presence of π-acceptor carbonyl ligands. A catalytic mechanism is proposed for 7 involving O–H oxidative addition of glycerol, β-hydride elimination, bicarbonate dehydroxylation, insertion and reductive elimination.
Catalytic transfer hydrogenation of CO2 from glycerol to afford formic and lactic acid is an attractive path to valorizing two waste streams. The process is significantly more thermodynamically favorable than direct CO2 hydrogenation.