Fire whirl is frequently observed in wildland fires, and may cause serious difficulty in firefighting owing to its significant turbulent flow. In this paper, the radiation of fire whirl is investigated through experiments using a fire whirl facility made up of an air curtain apparatus, with five different sizes of n-heptane pools (25, 30, 35, 40 and 45 cm). The flame contour was extracted by image processing. By using infrared methods, the flame emissivity of fire whirl at different heights for different pool diameters was measured, and thereby a correlation was developed between the flame emissivity and the flame diameter. The soot volume fraction in the luminous flame is estimated to range within 2.5 × 10−6 to 4.0 × 10−6, much higher than that of general heptane pool fires, which provides an explanation of the higher flame emissivity of fire whirl. The emissive power profile v. normalised height is deduced from flame emissivity and flame temperature data. A multizone flame model (in which each zone is assumed as a grey body) is used, based on the measured data of flame emissivity, to predict the radiation of fire whirl. Comparison between the predicted and measured data of radiative flux shows good agreement.
Laser power is a key factor in determining the microstructure and properties of metal materials prepared by additive manufacturing. This study selected the optimal laser power to enhance the corrosion resistance of maraging steel fabricated by direct energy deposition (DED). When the laser power was 3500 W, the corrosion current of the maraging steel was the lowest and the charge transfer resistance was the highest, demonstrating the best corrosion resistance. This is because at this laser power, the density of the maraging steel was the highest, reducing the penetration and diffusion of corrosive media. In addition, the content of high-valent Ni and Cr elements on the surface of the 3500 W maraging steel was higher than that of samples under other laser powers, indicating that the passivation film on its surface was denser than that of other samples, thereby slowing down the corrosion rate. This study proves that by adjusting the laser power, the density of the material and the composition of the surface passivation film can be precisely controlled, providing theoretical and experimental guidance for improving the corrosion resistance of maraging steel fabricated by DED.