梦 苏

Ms. 梦 苏


Research Focus & Metrics

Academic Career Length

1Year (2026-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
21 May 2026 in Materials
Verified
Journal Article
Open access
PDF file
楠丁楠 丁
楠 丁
ZCZhenyun Cheng
Zhenyun Cheng
JWJinghan Wu
Jinghan Wu
HLHua Lei
Hua Lei
梦苏梦 苏
梦 苏
BFBo Fu
Bo Fu
Sodium sulfate-activated slag cement is considered a highly promising low-carbon cementitious material; however, its application is limited by low early-age activation efficiency and slow strength development. This study aims to systematically elucidate the coupled regulatory mechanism of alkalinity (2% and 4% Na2O equivalent) and sodium sulfate dosage on the performance of alkali-activated slag (AAS). Under standard curing conditions (20 ± 2 °C, relative humidity ≥ 95%), the macroscopic properties of the samples (workability, setting time, and compressive strength) and the evolution of their microstructure (analyzed by XRD, FTIR, and SEM-EDS) were evaluated. The results indicate that the effect of sodium sulfate on alkali-activated slag (AAS) strongly depends on the alkalinity. Under low-alkalinity conditions (2% Na2O), sodium sulfate exhibits a synergistic activation effect by increasing the ionic concentration, promoting slag depolymerization and the nucleation of ettringite (AFt). Specifically, compared with the control, incorporating 6 wt% sodium sulfate (N2S6 mix) increased compressive strength by approximately 82% at 3 days and 21% at 28 days. In contrast, under high-alkalinity conditions (4% Na2O), excessive sodium sulfate (≥2 wt%) shows an inhibitory effect. This is likely because an excess of sodium sulfate interferes with the normal polymerization pathways of the aluminosilicate network, suppressing the formation of the primary C-(A)-S-H gel and thus significantly reducing later-age strength. Microstructural analysis revealed that the hydration products in the composite-activated system mainly consist of C-(A)-S-H gel, ettringite (AFt), monosulfate (AFm), and hydrotalcite. This study investigates the observed kinetic trends of anion-competitive hydration under different alkalinity conditions, providing a theoretical basis for the mix design of low-carbon alkali-activated materials and the valorization of coal chemical industrial salts.

2 September 2026 in Materials
Verified
Journal Article
Open access
PDF file
梦苏梦 苏
梦 苏
CCCan Chen
Can Chen
MCMeiqing Chen
Meiqing Chen
PWPeinian Wang
Peinian Wang
楠丁楠 丁
楠 丁
BFBo Fu
Bo Fu
To promote the high-value utilization of coal gasification slag (CGS) resources and mitigate the environmental issues caused by its accumulation, CGS was separated into five fractions by particle size (2.36–4.75 mm, 1.18–2.36 mm, 0.60–1.18 mm, 0.30–0.60 mm, and 0.15–0.30 mm) and subsequently ground into CGS powders (CGSPs). The physicochemical properties of both CGS and the obtained CGSP were systematically characterized, and the effects of CGSP on the hydration behavior and engineering performance of ordinary Portland cement (OPC) were investigated. The results revealed significant differences in physical properties and composition among the various particle-size fractions of CGS and their corresponding CGSP. When 40 wt.% CGSP was used to replace Portland cement, the C2.36 fraction exhibited the highest early-age compressive strength (16.91 MPa and 25.3 MPa at 3 d and 7 d, respectively), which is attributed to its favorable chemical composition and abundant glassy components. In contrast, the C0.6 fraction achieved the highest 28 d compressive strength (50.0 MPa). The C0.15 fraction showed the lowest strength at all ages, may be mainly due to its high residual carbon content and low reactivity. Overall, the compositional differences among CGS fractions of different particle sizes govern the formation and evolution of hydration products, and the proposed strategy of “classified grinding and quality-oriented utilization” provides an effective approach for the high-value application of CGS in cement-based materials.

22 October 2026 in Materials
Verified
Journal Article
Open access
PDF file
政屈政阳 屈
政阳 屈
YCYuanye Chen
Yuanye Chen
梦苏梦 苏
梦 苏
楠丁楠 丁
楠 丁
MCMeiqing Chen
Meiqing Chen
BFBo Fu
Bo Fu
Inorganic Softened sludge is a solid by-product generated during water treatment. Owing to its fine particle size and high calcium content, ISS has potential for use as a mineral admixture in cement-based materials. However, its specific role and underlying mechanisms in cementitious materials remain unclear. Therefore, this study systematically investigates the effects of different ISS replacement levels on the workability, mechanical properties, and hydration evolution of cement paste. The results showed that increasing the ISS replacement level progressively reduced the flowability of the paste and prolonged the setting time. Compared with the neat cement control, low ISS replacement levels (5–10%) increased the 3 days compressive strength, while causing only a slight reduction in the 28 days compressive strength; in contrast, high ISS replacement levels (15–30%) resulted in a pronounced decrease in compressive strength. Particle-size analysis showed that ISS had a smaller median particle size than OPC, suggesting a potential physical filling effect. Microstructural analyses indicated that ISS incorporation did not appreciably alter the types of major hydration products, while the detection of hemicarboaluminate (Hc) suggested that carbonate introduced by ISS may have participated in reactions involving aluminate phases. BSE/EDS observations revealed residual ISS-associated particles within the hydrated matrix, with Ca- and Si-enriched regions adjacent to some particles, consistent with the elemental composition of C-S-H-like hydration products. At low replacement levels, particle surface effects and possible physical filling effects may jointly contribute to the observed strength changes, potentially enhancing the early-age strength of the cementitious matrix.