In creep age forming (CAF), large integral panel components of high-strength aluminum alloy can be shaped and strengthened under external elastic loading at an elevated temperature through creep deformation and age hardening, simultaneously. However, the high ribbed structure on panel may induce stress concentration, inhomogeneous plastic deformation and even damage evolution on the bending rib, leading to the difficulty in controlling forming precision and material properties. Therefore, the generation and evolution of damage are necessary to be considered in the design of CAF. Taking 7050 aluminum alloy as the case material, the continuous and interrupted creep aging tests at 165 °C and three stress levels (300, 325, and 350 MPa) were conducted, and the corresponding material properties, precipitate, and damage microstructures were studied by mechanical properties tests, transmission electron microscope (TEM) and scanning electron microscope (SEM) characterizations. With the increase of stress level, the creep deformation occurs easier, the precipitates grow up faster, the creep damage occurs earlier, the growth rate and the size of microvoids increase, the mechanical properties decrease more rapidly, and the dominant mechanism of creep fracture changes from shear to microvoid coalescence. To simulate creep aging behavior with damage, a continuum damage mechanics (CDM) based model is calibrated and numerically implemented into ABAQUS solver via CREEP subroutine. The CAF of 7050 aluminum alloy panels with different height ribs were conducted by experiment and FE simulation. The forming process presents a typical stress relaxation phenomenon. The creep damage mainly occurs on the bending rib due to the severe stress concentration. With the increase of rib height, the creep strain and damage degree increase, but the springback decreases.
The effects of Mn/RE (Nd, Gd) multi-modification on the microstructure and high-temperature compressive creep properties of Mg–8.0Al alloys were investigated. The dominant intermetallic phases in the as-cast microstructure are β-Mg174Al12, Al2(Gd,Nd), Al11(Gd,Nd)3, Al8(Gd,Nd)Mn4, and Al10Mn2(Gd,Nd). The detailed structures of various intermetallics were revealed by TEM; the results indicate that Mn addition promotes grain refinement and facilitates the precipitation of lath-shaped and spherical β-Mg17Al12 in as-cast Mg–Al–RE alloys, resulting in increases in the tensile strength and elongation of the 1.0Mn alloy by 26.5% and 92.1%, respectively. Additionally, thermally stable micron-scale Al8(Gd,Nd)Mn4 and Al12(Gd,Nd)2Mn5, along with dynamically precipitated spherical nano-sized AlGd and AlNd particles in the α-Mg matrix, were innovatively observed in compression-crept specimens tested at 200 °C and 60 MPa; these phases play a key role in improving high-temperature creep resistance. A significant finding is that excessive Mn addition deteriorates creep performance, which is attributed to excessive grain refinement and the consequent increase in the contribution of grain boundary sliding during creep. However, the negative effect of grain boundary sliding—caused by grain refinement—on creep performance can be balanced by the strengthening effect of Al–Mn–Gd phases and the dynamic precipitation of nanoscale Al–RE particles. This paper provides new insights for designing Mg–Al–Nd–Gd–Mn alloys with both excellent high-temperature creep resistance and significantly enhanced mechanical properties.