Thermal degradation on PL intensity of as-prepared and N2-treated Sr2Si5N8:Eu2+ phosphors with heating (heating from 30 °C to 300 °C) and cooling (from 300 °C to 30 °C). Insets are their photographs phosphor powders excited in a 365 nm-UV box.
Chlorides of NH4Cl and SrCl2 and fluorides of AlF3 and SrF2 were added to raw materials acting as the flux for preparing the SrSi2O2N2:Eu2+ phosphor. The effects of the fluxes on the phase formation, particle morphology, particle size, and photoluminescence properties were investigated. The results revealed that particle size, particle morphology and photoluminescence intensity were largely dominated by the type of the flux material and its adding amount. The chloride-based flux was found to favor the formation of the SrSi2O2N2:Eu2+ phase. Among the chloride-based fluxes, the sample added with the SrCl2 flux presented the narrow particle distribution and cleaner surface, with enhanced emission intensity and an increased external quantum efficiency by 68% and 22%, respectively, compared with those of the sample without any flux adding.
Cellulose nanofibers were modified by TiO2 gel layer (~25 nm in thickness) via hydrolysis reaction on the surface of the cellulose nanofibers. After the TiO2 coating, the surface charge of the nanofiber dramatically changed from negative to positive. A high efficiency (~100%) of capturing negatively charged Au nanoparticles (5 nm) was successfully obtained by effectively utilizing the electrostatic interaction of surface charge between the TiO2-coated cellulose nanofibers and Au nanoparticles. Therefore, this technique of surface modification will be potentially used in improving filtration efficiency for membrane applications.
The phosphor deposits of the β-sialon:Eu2+ mixed with various amounts (0–1 g) of the SnO2 nanoparticles were fabricated by the electrophoretic deposition (EPD) process. The mixed SnO2 nanoparticles was observed to cover onto the particle surfaces of the β-sialon:Eu2+ as well as fill in the voids among the phosphor particles. The external and internal quantum efficiencies (QEs) of the prepared deposits were found to be dependent on the mixing amount of the SnO2: by comparing with the deposit without any mixing (48% internal and 38% external QEs), after mixing the SnO2 nanoparticles, the both QEs were improved to 55% internal and 43% external QEs at small mixing amount (0.05 g); whereas, with increasing the mixing amount to 0.1 and 1 g, they were reduced to 36% and 29% for the 0.1 g addition and 15% and 12% l QEs for the 1 g addition. More interestingly, tunable color appearances of the deposits prepared by the EPD process were achieved, from yellow green to blue, by varying the addition amount of the SnO2, enabling it as an alternative technique instead of altering the voltage and depositing time for the color appearance controllability.
6 April 2020 in Journal of the American Ceramic Society