Pure chitosan membranes present insufficient mechanical properties and a high swelling ratio, which limits their application in biomedical field. In this study, silk microfibers were obtained by chemical hydrolysis, and a novel type of chitosan/silk microfiber (CS/mSF) blended membrane was reported and its multiple physical properties were evaluated. The mechanical properties were significantly improved after blending silk microfibers with a chitosan matrix, while the swelling ratio was decreased. Observation of the surface microstructures of the blended membranes via scanning electron microscopy showed abundant embedding of mSF into the CS matrix, as well as connections among mSF. In vitro cytocompatibility was also investigated, and the blended membranes exhibited significant cytocompatibility, which was demonstrated by cell proliferation and cell morphology. Furthermore, the in vivo healing effects of the blended membrane as a wound dressing were determined on a full-thickness skin wound model of rats. Animal studies revealed that the membranes containing mSF exhibited increased wound healing efficiency compared with pure CS membranes and treatment without wound dressing. From an examination of histological changes, a higher level of epithelialization and collagen formation was observed with treatment of CS/mSF blended membranes after a 21 day repair period. In conclusion, our results indicated that the blended membranes with CS and mSF might be a potential candidate material for wound healing.
An environmental physical method described herein was developed to improve the tensile properties of Bombyx mori cocoon sericin films, by using the plasticizer of glycerol, which has a nontoxic effect compared with other chemical crosslinkers. The changes in the tensile characteristics and the structure of glycerolated (0–40 wt% of glycerol) sericin films were investigated. Sericin films, both in dry and wet states, showed enhanced tensile properties, which might be regulated by the addition of different concentrations of glycerol. The introduction of glycerol results in the higher amorphous structure in sericin films as evidenced by analysis of attenuated total reflection Fourier transform infrared (ATR-FTIR) spectra, thermogravimetry (TGA) and differential scanning calorimetry (DSC) curves. Scanning Electron Microscopy (SEM) observation revealed that glycerol was homogeneously blended with sericin molecules when its content was 10 wt%, while a small amount of redundant glycerol emerged on the surface of sericin films when its content was increased to 20 wt% or higher. Our results suggest that the introduction of glycerol is a novel nontoxic strategy which can improve the mechanical features of sericin-based materials and subsequently promote the feasibility of its application in tissue engineering.
In order to use a simple and ecofriendly method to prepare porous silk scaffolds, aqueous silk fibroin solution (ASF) was extracted from silk gland of 7-day-old fifth instar larvae of Bombyx mori (B. mori). SDS-page analysis indicated that the obtained fibroin had a molecular weight higher than 200 kDa. The fabrication of porous scaffolds from ASF was achieved by using the freeze-drying method. The pore of porous scaffolds is homogenous and tends to become smaller with an increase in the concentration of ASF. Conversely, the porosity is decreased. The porous scaffolds show impressive compressive strength which can be as high as 6.9 ± 0.4 MPa. Furthermore, ASF has high cell adhesion and growth activity. It also exhibits high ALP activity. This implies that porous scaffolds prepared from ASF have biocompatibility. Therefore, the porous scaffolds prepared in this study have potential application in tissue engineering due to the impressive compressive strength and biocompatibility.