The Ti-18Zr-15Nb shape memory alloys are a new material for medical implants. The regularities of phase transformations during heating of this alloy in the coarse-grained quenched state and the nanostructured state after high-pressure torsion have been studied. The specimens in quenched state (Q) and HPT state were annealed at 300–550 °C for 0.5, 3, and 12 h. The α-phase formation in Ti-18Zr-15Nb alloy occurs by C-shaped kinetics with a pronounced peak near 400–450 °C for Q state and near 350–450 °C for HPT state, and stops or slows down at higher and lower annealing temperatures. The formation of a nanostructured state in the Ti-18Zr-15Nb alloy as a result of HPT suppresses the β→ω phase transformation during low-temperature annealing (300–350 °C), but activates the β→α phase transformation. In the Q-state the α-phase during annealing at 450–500 °C is formed in the form of plates with a length of tens of microns. The α-phase formed during annealing of nanostructured specimens has the appearance of nanosized particle-grains of predominantly equiaxed shape, distributed between the nanograins of β-phase. The changes in microhardness during annealing of Q-specimens correlate with changes in phase composition during aging.
Biomedical Ti-22Nb-6Zr, Ti-18Zr-15Nb, and Ti-41Zr-12Nb (at.%) shape memory alloys were subjected to cold rolling (CR) and subsequent post-deformation annealing (PDA). The evolutions of phase and structure states, crystallographic texture, and crystallographic limit of recovery strain were studied using EBSD, TEM, and XRD analyses. The study found that CR (e = 1.5) and PDA at 800 °C for 30 min results in fine- and coarse-grained structures. Severe CR (e = 3.0) and PDA at 550 °C for 5 min results in a recrystallized, equiaxed, predominantly ultrafine-grained structure of the β-phase with a small amount of low-angle boundaries. Increasing the degree of CR from moderate (e = 0.3) to severe (e = 3.0) results in a favorable strong {111}ββ recrystallization texture. Alloys with low Zr content are more susceptible to this type of crystallographic texture formation during TMT, primarily due to a higher Nb content. The Ti-41Zr-12Nb alloy shows the highest crystallographic limit of recovery strain (εrmax ≈ 6%). The limit decreases to ≈5% (for Ti-18Zr-15Nb) and ≈3% (for Ti-22Nb-6Zr) when transitioning from high- to low-Zr alloys. The transition of Ti-Zr-Nb alloys from coarse-grained to ultrafine-grained structures of the β-phase and a decrease in grain size do not affect the crystallographic limit of recovery strain in the studied grain size ranges.
1 July 2020 in Russian Journal of Non-Ferrous Metals
Multicomponent alloys without a base element, also known as highly entropic alloys (HEAs), are of great interest for research. The microstructure of the Fe
1 July 2021 in Russian Journal of Non-Ferrous Metals