In this study, hectorite intercalated with octadecyl trimethylammonium ions was synthesized via one-pot synthesis, and the octadecyl trimethylammonium-modified hectorite was used as an adsorbent to remove phenol from an aqueous solution. The pH and content of the adsorbent were studied to determine the optimized conditions for the adsorption of phenol. The phenol removal rate attained for 50 mL of 100 mg/L initial phenol solution at pH 12 was about 92.3% when 0.5 g of adsorbent was used. As for the adsorption isotherm, the Langmuir and Freundlich models were appropriate. The adsorption kinetics were in accordance with the pseudo-second-order model, and the activation energy (Ea) was about 11.15 kJ/mol. The modified hectorite could be recycled and reused, maintaining a high adsorption amount after five cycles.

22 July 2026 in Preprints.org
Verified
Preprint
Open access
PDF file
YZYunhan Zhao
Yunhan Zhao
WXWang xueting Wang xueting
Wang xueting Wang xueting
JCJinyang Chen
Jinyang Chen
Hectorite intercalated with octadecyl trimethylammonium ions was synthesized with one-pot synthesis and the octadecyl trimethylammonium modified hectorite was used as adsorbent to remove phenol from aqueous solution. The pH and content of adsorbent were studied to obtain optimized condition to the adsorption of phenol. As for the 50 ml of 100 mg/L initial phenol solution at pH 12, the phenol removal rate attains about 92.3% when 0.5 g adsorbent is used. As for the adsorption isotherm, the Langmuir and Freundlich model were appropriate. The adsorption kinetic was in accord with the pseudo-second-order and the activation energy (Ea) was about 11.15 kJ/mol. The modified hectorite could be recycled and reused, maintaining a high adsorption amount after five times.