1,5-Dimethyl-4-((2-methylbenzylidene)amino)-2-phenyl-1H-pyrazol-3(2H)-one (DMPO) was synthesized to be evaluated as a corrosion inhibitor. The corrosion inhibitory effects of DMPO on mild steel in 1.0 M HCl were investigated using electrochemical impedance spectroscopy (EIS), potentiodynamic polarization, open circuit potential (OCP) and electrochemical frequency modulation (EFM). The results showed that DMPO inhibited mild steel corrosion in acid solution and indicated that the inhibition efficiency increased with increasing inhibitor concentration. Changes in the impedance parameters suggested an adsorption of DMPO onto the mild steel surface, leading to the formation of protective films. The novel synthesized corrosion inhibitor was characterized using UV-Vis, FT-IR and NMR spectral analyses. Electronic properties such as highest occupied molecular orbital energy, lowest unoccupied molecular orbital energy (EHOMO and ELUMO, respectively) and dipole moment (μ) were calculated and discussed. The results showed that the corrosion inhibition efficiency increased with an increase in the EHOMO values but with a decrease in the ELUMO value.
1 February 2015 in Engineering and Technology Journal
The current study deals with hazards and safety precautions of some pharmaceutical and cosmetic creams used extensively in Iraq. UV absorption - related diseases of these products and people unawareness of side effects and the weak quality control are other reasons for conducting such study. Spectral study of fourteen pharmaceuticals and cosmetics was carried out within a wavelength range of (200 – 700)nm. The maximum absorption percentage of UV region was 5% for Tetraderm and and 3.66% for Nivea cream.
1 February 2013 in Engineering and Technology Journal
Metal samples such as Copper and Aluminum and alloy as Brass were prepared and machined as discs (plane sample) and as a half rings (curvature sample). The samples were polished by using metallographic paper with different grades. The micro roughness and the initial weight were measured for all samples before wear tests, and then the samples were subjected to wear testing system under lubricated condition, fixed normal load of 15N, sliding time 30 min and sliding speed of 750 rpm. During the running of wear testing system the temperature of the samples were measured .The wear rate was calculated by employing the weighing method. It is clear from the results that micro roughness values increasing leads to increase in weight loss , wear rate and the temperature of samples .The effect of sample shape on weight loss , wear rate and sample heat is also obvious when noticing that the different measurements of weight loss, wear rate and sample heat of curvature samples are higher than that of plane samples .