Gemstone commercial is a high revenue for Thailand especially ruby and sapphire. Moreover, Phrae is a potential gem field located in the northern part of Thailand. The studies of spectroscopic properties are mainly to identify gemstone using advanced techniques (e.g. UV-Vis-NIR spectrophotometry, FTIR spectrometry and Raman spectroscopy). Typically, UV-Vis-NIR spectrophotometry is a technique to study the cause of color in gemstones. FTIR spectrometry is a technique to study the functional groups in gem-materials. Raman pattern can be applied to identify the mineral inclusions in gemstones. In this study, the natural sapphires from Ban Bo Kaew were divided into two groups based on colors including blue and green. The samples were analyzed by UV-Vis-NIR spectrophotometer, FTIR spectrometer and Raman spectroscope for studying spectroscopic properties. According to UV-Vis-NIR spectra, the blue sapphires show higher Fe3+/Ti4+ and Fe2+/Fe3+ absorption peaks than those of green sapphires. Otherwise, green sapphires display higher Fe3+/Fe3+ absorption peaks than blue sapphires. The FTIR spectra of both blue and green sapphire samples show the absorption peaks of –OH,-CH and CO2. The mineral inclusions such as ferrocolumbite and rutile in sapphires from this area were observed by Raman spectroscope. The spectroscopic properties of sapphire samples from Ban Bo Kaew, Phrae Province, Thailand are applied to be the specific evidence for gemstone identification.
17 December 2018 in Journal of Physics: Conference Series
Corundum (ruby & sapphire) consists of Al2O3 and trace elements relating to the cause of color such as Cr, Fe, and Ti. Irradiation is one of gemstone enhancements for improving their color. The aim of this study is focused on the oxidation state of Fe ions that concern with the cause of yellow color in irradiated sapphire by XAS technique. In this study, natural sapphire samples from Sri Lanka were collected. The samples were irradiated with high energy electron beam at 40,000 kGy, 60,000 kGy, and 80,000 kGy. XAS technique was emphasized on Fe Kedge XANES spectra. The Fe-chemical standard includes FeO and Fe2O3 referred to Fe 2+ and Fe 3+ oxidation states, respectively. According to the results, the absorption edge position of the Fe K-edge XANES spectra detected from the samples is similar to the position from Fe2O3. Moreover, the linear combination fitting of Fe ions in the samples compared with the Fechemical standard shows that the cause of yellow color on irradiated sapphire samples could be affected by Fe 3+ concerning with the UV-Vis-NIR spectra. Hence, it could be summarized that the increasing of yellow color in irradiated sapphires is due to the increasing of high energy electron doses and the ratio of Fe 3+ oxidation state on the sample surface.
The blue color of sapphire is associated with Fe and Ti impurities that replace Al3+ in the corundum structure. Typically, sapphire color depends on its geological origin, such as basaltic or metamorphic localities, and the blue hue can change after heating in an oxidizing environment. Nonetheless, previous studies on the blue color mechanism have left some questions unanswered. Therefore, this research examines how the oxidation states of Fe and Ti influence sapphire color and explores the mechanism of blue coloration before and after heating in oxidizing and reducing atmospheres. This study involved collecting sapphire samples from various gem localities, including basalt-related sapphires from Kanchanaburi, Thailand, and metamorphic-related sapphires from Sri Lanka. The samples were heated in an oxidizing environment at 1100 °C, then at either 1300 °C or 1500 °C in both oxidizing and reducing environments. As a result, after heating under an oxidizing environment at either 1300 °C or 1500 °C, the basalt-related sapphires turned from light blue to pale blue, and the metamorphic-related ones turned colorless. The Fe3+-Ti4+ mixed acceptor states decreased because an electron from the valence band recombined with a hole in the color center during heating. On the other hand, the blue color observed in sapphire samples after heating in a reducing environment at 1300 °C could be explained by electrons being depleted from the hole color center associated with Fe3+-Ti4+ mixed acceptor states within the energy band gap, thereby making them ready to receive electrons from the valence band upon optical excitation. Therefore, it can be concluded that the blue color mechanism in sapphires before and after heating under different atmospheric environments can be explained by an energy-band model involving the presence or absence of Fe3+-Ti4+ mixed acceptor states, as well as a hole color center within the energy band gap. Furthermore, after heating at 1300 °C and 1500 °C in a reducing environment, the oxidation state of Fe gradually decreases from 3+ to 2+. The samples turn black upon heating to 1500 °C, indicating that Fe2+-Ti4+ is responsible for the black color rather than the blue observed in sapphires.