To ensure the highest safety standards in modern automobiles, the industry is constantly adopting zero-defect frameworks, such as AEC-Q100, which aims for defective-parts-per-billion (DPPB) or grade-0 level reliability standards in automotive integrated-circuit (IC) packages. Most contemporary wire-bonded packages use either pure copper (Cu) or palladium (Pd)-coated copper (PCC) wires bonded to aluminum (Al) bond pads as interconnections. This choice is made due to their lower cost and superior electrical and mechanical performance, compared to traditional gold wire-based devices. However, these Cu–Al wire-bonded interconnections are prone to ion-induced lift-off/open-circuit corrosion failures when exposed to even trace amounts (<20 ppm) of extrinsic and/or intrinsic halide (Cl− and Br−) contaminants, decreasing device longevity. This study investigates corrosion failure mechanisms in Cu and PCC wire-based devices by subjecting non-encapsulated devices to a highly accelerated aqueous-immersion screening test containing 100 ppm chloride (Cl−), 100 ppm bromide (Br−), and a mixed-ion solution (MX: Cl− + Br−). The screening results indicate that even control PCC-Al devices with a Pd overlayer can be susceptible to Cl− and Br− induced corrosion, with 21 ± 1.6% lift-off failures in MX-solution. In contrast, applying a novel Cu-selective passivation reduced lift-off to 3.3 ± 0.6% and introducing phosphonic-acid-based inhibitor into the MX solution eliminated lift-off failures, demonstrating markedly improved reliability.
Copper–aluminum (Cu-Al) wire-bonded devices are widely used in microelectronic packaging; however, corrosion at exposed Cu-Al bimetallic interfaces can lead to Al pad degradation, undercutting, and eventual ball-bond lift-off or open-circuit failure under humid, halide-contaminated conditions. This work presents a scalable post-wire-bond wet-chemical passivation process using octadecylphosphonic acid (ODPA) to simultaneously modify exposed Cu/Pd-coated Cu (PCC) and Al surfaces. The passivation process includes a hydroxylation pretreatment to generate reactive oxide/hydroxide surface sites, followed by ODPA treatment and solvent rinsing to remove weakly adsorbed species. Surface modification was evaluated using contact-angle measurements, reflection–absorption infrared spectroscopy (RAIRS), atomic force microscopy (AFM), and X-ray photoelectron spectroscopy (XPS). ODPA treatment increased the water contact angle on Cu and Al, confirming a substantial increase in surface hydrophobicity following coating formation. RAIRS identified ODPA-associated aliphatic C-H bands, AFM showed treatment-induced nanoscale surface changes, and XPS supported metal–oxygen–phosphorus interfacial bonding. Under aggressive 100 ppm chloride-ion immersion, ODPA passivation strongly suppressed corrosion-induced ball-bond lift-off across both device platforms. Lift-off decreased from 99.0% to 0.73% for Cu-Al devices and from 23.3% to 0.42% for PCC-Al devices. Collectively, these findings establish an effective, process-compatible post-wire-bond strategy for substantially protecting corrosion-susceptible interfaces and thereby improving the reliability of wire-bonded interconnects in halide-containing environments.