Al–Mg–Si alloys are usually formed into their final shape by rolling or extrusion. After extrusion, the aluminium profiles are usually straightened, causing the material to be subjected to a small plastic deformation. This study demonstrates the positive effect on strength that can be obtained from such small deformation levels or from only elastically straining the material. Elastic straining of a lean Al–Mg–Si alloy, when performed immediately after solution heat treatment, enhances the material yield strength after artificial ageing to T6. Transmission electron microscopy shows that this effect can be attributed to a higher number density and finer dispersion of the age-hardening precipitate needles. Furthermore, introducing a small plastic deformation of 1% after solution heat treatment results in a comparable strength increase to elastically straining the material. In this case, however, the strength increase is due to the increased dislocation density, which compensates for a lower density of precipitate needles. Finally, by combining plastic deformation with a succeeding elastic strain, we demonstrate how elastic strain can cause an on-set of dislocation cell formation in this material.
Four Al-Mg-Si alloys, three of them with additions of scandium or scandium and zirconium, were cast, homogenised at 550 °C, and precipitation hardened at 175 °C. For the alloy with the highest Sc content, significant discontinuous precipitation of Al3Sc took place during cooling after casting. Homogenisation for 1 h led to the formation of Al3Sc or Al3(Sc,Zr) dispersoids. The Al3(Sc,Zr) dispersoids were found in higher number densities than the Al3Sc dispersoids, and the latter were not stable for longer homogenisation times. TEM observations indicate that the Al3Sc or Al3(Sc,Zr) dispersoids are not preferred nucleation sites for metastable (Mg,Si) particles. The precipitation hardening behaviour of the Al-Mg-Si alloys was not altered by the Sc or Sc+Zr additions.