Representative Publications

View All Publications
12 March 2019 in Crystals
Verified
Journal Article
Open access
PDF file
YHYoosung Ha
Yoosung Ha
AKAkihiko Kimura
Akihiko Kimura
The effect of cold rolling on the recrystallization behavior of Al-free and Al-added 15Cr-oxide dispersion strengthened (ODS) ferritic steels was investigated. The recrystallization of both steels are enhanced by cold rolling. The Al-free ODS steel with finer oxide particles is harder to recrystallize than Al-added ODS steel with coarser oxide particles. The effect of Al addition on the recrystallization behavior is evident. It is estimated that the recrystallization temperature of Al-free and Al-added 15Cr-ODS ferritic steel is 900 °C and 1250 °C with the annealing period of 1 h. In Al-free ODS steel, a small hardening was observed in the temperature range between 850 °C and 1200 °C, while no such phenomenon was observed in Al-added ODS steel, which is indicative of retardation of recovery by finely dispersed oxide particles. Oxide particle growth is mostly dependent on annealing temperature, while recrystallization and grain growth are controlled by not only the temperature, but the cold rolling ratio, which alters the multiple factors such as dislocation density, initial grain shape and oxide particle dispersion morphology. The cold rolling direction also influences the grain morphology and grain orientation in Al-added ODS steel, and the second rolling in a perpendicular direction to the first cold rolling direction induces the rotation of the grains from to . The recrystallization temperature is not significantly changed by the cold rolling direction. Recrystallization after cold rolling appears to increase the {111} grain orientation on the cold rolled specimen surface.

2 August 2018 in Journal of Pressure Vessel Technology
Verified
Journal Article
Closed access
PDF file
YHYoosung Ha
Yoosung Ha
TTTohru Tobita
Tohru Tobita
TOTakuyo Ohtsu
Takuyo Ohtsu
HTHisashi Takamizawa
Hisashi Takamizawa
YNYutaka Nishiyama
Yutaka Nishiyama
The applicability of miniature compact tension (Mini-C(T)) specimens to fracture toughness evaluation of neutron-irradiated reactor pressure vessel (RPV) steels was investigated. Three types of RPV steels neutron-irradiated to a high-fluence region were prepared and manufactured as Mini-C(T) specimens according to Japan Electric Association Code (JEAC) 4216-2015. Through careful selection of the test temperature by considering previously obtained mechanical properties data, valid fracture toughness, and reference temperature (To) was obtained with a relatively small number of specimens. Comparing the fracture toughness and To values determined using other larger specimens with those determined using the Mini-C(T) specimens, To values of both unirradiated and irradiated Mini-C(T) specimens were found to be the acceptable margin of error. The scatter of 1T-equivalent fracture toughness values of both unirradiated and irradiated materials obtained using Mini-C(T) specimens did not differ significantly from the values obtained using larger specimens. The correlation between the Charpy 41 J transition temperature (T41J) and the To values agreed very well with that of the data in the literature, regardless of specimen size and fracture toughness of the materials before irradiation. Based on these findings, it was concluded that Mini-C(T) specimens can be applied to fracture toughness evaluation of neutron-irradiated materials without significant specimen size dependence.

1 December 2019 in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
Verified
Journal Article
Closed access
YHYoosung Ha
Yoosung Ha
HTHisashi Takamizawa
Hisashi Takamizawa
JKJinya Katsuyama
Jinya Katsuyama
SHSatoshi Hanawa
Satoshi Hanawa
YNYutaka Nishiyama
Yutaka Nishiyama

23 November 2021 in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
Verified
Journal Article
Closed access
KIKeiko Iwata
Keiko Iwata
HTHisashi Takamizawa
Hisashi Takamizawa
YHYoosung Ha
Yoosung Ha
MSMasaki Shimodaira
Masaki Shimodaira
YOYoshihiro Okamoto
Yoshihiro Okamoto
YNYutaka Nishiyama
Yutaka Nishiyama

2 December 2022 in Journal of Pressure Vessel Technology
Verified
Journal Article
Closed access
PDF file
YHYoosung Ha
Yoosung Ha
TTTohru Tobita
Tohru Tobita
HTHisashi Takamizawa
Hisashi Takamizawa
JKJinya Katsuyama
Jinya Katsuyama
The fracture toughness in the heat-affected zone (HAZ), which is located under the weld overlay cladding on the inner surface of the reactor pressure vessel (RPV), was evaluated by considering the inhomogeneous microstructures of the HAZ. In this regard, 0.4T-C(T) specimens and miniature C(T) (Mini-C(T)) specimens were manufactured to clarify the effect of the HAZ on fracture toughness. First, the fracture toughness was evaluated using 0.4T-C(T) specimens targeted on microstructural distribution due to the cladding bead location. The reference temperature (To) of HAZ at middle region of cladding bead was 12 °C higher than that at overlap cladding beads. Second, the fracture toughness was evaluated using Mini-C(T) specimens focused on the microstructural difference with distance from the boundary between the cladding and the base metal. The To value of the central position located at 3–7 mm from the boundary between the cladding and the base metal was higher than those of the other positions in HAZ. However, the To values of HAZ for both 0.4T-C(T) and Mini-C(T) specimens were significantly lower than that of the base metal at a quarter thickness by 40–60 °C. Compared with the literature data that indicated fracture toughness at the inner surface without overlay cladding and the base metal at a quarter thickness, this study concluded that the HAZ under the overlay cladding showed no detrimental effect on the conservatism of the structural integrity assessment of RPV steel.

28 April 2026 in SSRN Electronic Journal
Verified
Preprint
Open access
MNMartin Negyesi
Martin Negyesi
YHYoosung Ha
Yoosung Ha
VLValéry Lacroix
Valéry Lacroix
PHPetr Haušild
Petr Haušild
This study is concerned with the evaluation of yield and tensile strengths of nuclear power plant (NPP) structural components by on-site measurement of instrumented indentation technique (IIT). Yield and tensile strengths were measured on the outer surface of Lemoniz NPP reactor pressure vessel (RPV) to primary piping joint segment employing IIT at ambient temperature. Tensile tests of specimens extracted from the joint were carried out at the reactor operating temperature. Through-thickness variation in yield and tensile strengths was assessed by the tensile tests and micro-hardness testing on joint axial cross section. The results of IIT were extrapolated to the reactor operating temperature by using strength-temperature correlations based on tabulated data of American Society of Mechanical Engineers (ASME), Boiler and Pressure Vessel Code (BPVC), Section II, Part D and compared to the tensile test results. A satisfactory agreement has been achieved, mainly for base materials. Larger deviation between surface IIT and bulk tensile test data has been observed for weldments. The through-thickness variation in yield and tensile strengths was within 5 %. It was concluded that surface IIT measurement carried out during reactor shut-down condition could estimate bulk equivalent yield and tensile strengths of RPV nozzle to primary piping joint materials at the reactor operating temperature by about 10 % deviation provided temperature extrapolation accurate enough would be applied.