Junfeng Cheng

Junfeng Cheng


Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2021 in Journal of Renewable Materials
Verified
Journal Article
Open access
ZCZheng Cao
Zheng Cao
YZYang Zhang
Yang Zhang
KLKeming Luo
Keming Luo
YWYinqiu Wu
Yinqiu Wu
HGHongxin Gao
Hongxin Gao
LZLei Zhang
Lei Zhang
The preparation and application of functional hydrogels based on natural polysaccharides have always been a hot research topic. In this study, using acrylamide (AM) monomer, N, N'-methylene bisacrylamide (MBA) as cross-linking agent, potassium persulfate (K2S2O8) as initiator, in the presence of natural polysaccharide sodium alginate (SA), the PAM/SA hydrogel was prepared by free radical polymerization. Fourier transform infrared spectroscopy (FT-IR), swelling performance tests, scanning electron microscope (SEM), thermogravimetric analysis (TGA), UV-visible spectrophotometer, mechanical property measurements were carried out to analyze the composition, morphology, and performance of the hydrogels. The swelling behavior, dye adsorption performance, and the mechanical properties of PAM/SA hydrogels before and after Fe3+ adsorption were studied. The experimental results showed that the introduction of SA with 4.7%, 7.8%, and 10.3% effectively improved the mechanical and dye adsorption properties of PAM composite hydrogels. The adsorption capacity of PAM/4.7%SA and PAM/10.3%SA hydrogels at equilibrium can reach 40.01 and 44.02 mg/g for methylene blue, which is higher than the value 13.58 mg/g of pure PAM hydrogel. The compressive strength of pure PAM hydrogel is 0.124 MPa. When the SA content is 4.7%, 7.8%, and 10.3%, the compressive strength of the PAM/SA hydrogel was corresponding to 0.130 MPa, 0.134 MPa, and 0.152 MPa, respectively. Fe3+ was introduced into the PAM/SA hydrogels, and PAM/SA/Fe3+ double-network hydrogels with excellent mechanical properties could be prepared by adjusting the SA content (4.7%, 7.8%, and 10.3%), soaking time (1 h, 2 h, 3 h, 4 h, 5 h, 6 h), and Fe3+ concentration (4.76%, 7.41%, 9.09%, and 13.04%). Under the same Fe3+ concentration of 9.09% and adsorption time of 4 h, the compressive strengths of the PAM/4.7%SA, PAM/7.8%SA, and PAM/10.3%SA hydrogels could reach 0.354 MPa, 0.767 MPa, and 0.778 MPa, respectively.

15 January 2019 in Soft Matter
Verified
Journal Article
Closed access
PDF file
ZCZheng Cao
Zheng Cao
YCYuyuan Chen
Yuyuan Chen
CZCheng Zhang
Cheng Zhang
JCJunfeng Cheng
Junfeng Cheng
DWDun Wu
Dun Wu
ZFZhisheng Fu
Zhisheng Fu
Polystyrene modified bismuth oxide particles (PS@Bi2O3) were prepared and characterized by Fourier transform infrared spectroscopy (FT-IR) and scanning electron microscopy (SEM).

25 March 2021 in ACS Omega
Verified
Journal Article
Open access
ZCZheng Cao
Zheng Cao
GLGuangwei Lu
Guangwei Lu
HGHongxin Gao
Hongxin Gao
ZXZhiyu Xue
Zhiyu Xue
KLKeming Luo
Keming Luo
MLMing Luo
Ming Luo
In this study, using molybdenum sulfide (MoS2) as laser-sensitive particles and poly(propylene) (PP) as the matrix resin, laser-markable PP/MoS2 composite materials with different MoS2 contents ranging from 0.005 to 0.2% were prepared by melt-blending. A comprehensive analysis of the laser marking performance of PP/MoS2 composites was carried out by controlling the content of laser additives, laser current intensity, and the scanning speed of laser marking. The color difference test shows that the best laser marking performance of the composite can be obtained at the MoS2 content of 0.02 wt %. The surface morphology of the PP/MoS2 composite material was observed after laser marking using a metallographic microscope, an optical microscope, and a scanning electron microscope (SEM). During the laser marking process, the laser energy was absorbed and converted into heat energy to cause high-temperature melting, pyrolysis, and carbonization of PP on the surface of the PP/MoS2 composite material. The black marking from carbonized materials was formed in contrast to the white matrix. Using X-ray diffraction (XRD), Fourier transform infrared (FT-IR) spectroscopy, and Raman spectroscopy, the composite materials before and after laser marking were tested and characterized. The PP/MoS2 composite material was pyrolyzed to form amorphous carbonized materials. The effect of the laser-sensitive MoS2 additive on the mechanical properties of composite materials was investigated. The results show that the PP/MoS2 composite has the best laser marking property when the MoS2 loading content is 0.02 wt %, the laser marking current intensity is 11 A, and the laser marking speed is 800 mm/s, leading to a clear and high-contrast marking pattern.

27 November 2019 in ACS Omega
Verified
Journal Article
Open access
CZCheng Zhang
Cheng Zhang
YDYankai Dai
Yankai Dai
GLGuangwei Lu
Guangwei Lu
ZCZheng Cao
Zheng Cao
JCJunfeng Cheng
Junfeng Cheng
CLChunlin Liu
Chunlin Liu
In this work, using ferroferric oxide (Fe3O4) and zirconium oxide (ZrO2) as laser-sensitive particles and thermoplastic polyurethane (TPU) as the matrix resin, a series of TPU/Fe3O4/ZrO2 composites were prepared by melt blending, and the effect of the laser marking additive content, composition, and laser marking parameters on the laser marking properties of composites was investigated. The laser marking mechanism of Fe3O4/ZrO2 additives and the role of each component in TPU laser marking were studied by metallographic microscopy, color difference test, scanning electron microscopy, and Raman spectroscopy. Fe3O4 nanoparticles as a laser sensitizer component, on the one hand, can act as a pigment to make the TPU substrate black and, on the other hand, can absorb laser energy to contribute to the formation of laser markings on TPU composite surfaces. In addition, the introduction of ZrO2 nanoparticles can help absorb the laser energy, while the contrast can be improved to enhance the laser marking performance of the TPU composite. Through thermogravimetric analysis, the changes in the thermally stable properties of TPU composites before and after laser marking were investigated, and the results indicated that Fe3O4/ZrO2 nanoparticles can absorb the laser energy, causing melting and pyrolysis of the TPU backbone at a high temperature, to produce a gaseous product resulting in foaming. Finally, the high-contrast and light-colored markings were formed on the black TPU composite surface. This work provides a facile method for producing high-contrast and light-colored markings on the dark TPU composite surface.

25 January 2024 in Journal of Porous Materials
Verified
Journal Article
Closed access
PDF file
XZXin Zhou
Xin Zhou
SLSiying Liu
Siying Liu
YHYumeng Hu
Yumeng Hu
JHJiatong He
Jiatong He
WZWeiyue Zhang
Weiyue Zhang
JCJunfeng Cheng
Junfeng Cheng

2 February 2019 in Polymers
Verified
Journal Article
Open access
PDF file
ZCZheng Cao
Zheng Cao
YCYuyuan Chen
Yuyuan Chen
DLDan Li
Dan Li
JCJunfeng Cheng
Junfeng Cheng
CLChunlin Liu
Chunlin Liu
A SiO2 microsphere imprinted by phosphate ions was prepared with the use of phosphate ion as the template molecule and tetraethoxysilane as the precursor. Thereafter, the imprinted SiO2 microspheres were modified with 3-(trimethoxysilyl)propyl methacrylate (TMSPMA@SiO2), followed by introducing the double bond. In the presence of TMSPMA@SiO2, using N-isopropylacrylamide as monomer, and potassium persulfate as initiator, polymer/inorganic hybrid particles (PNIPAM/SiO2) were prepared. Fourier transform infrared spectroscopy, thermogravimetric analysis, nitrogen adsorption-desorption test, and transmission electron microscope were employed for the characterization of molecular imprinted SiO2 microspheres and PNIPAM/SiO2 hybrid particles. The effects of phosphate concentration, pH value, and adsorption temperature on the phosphate binding properties of PNIPAM/SiO2 hybrid particles were studied by UV-vis spectrophotometer. The experimental results shed light on the fact that the PNIPAM structure is beneficial for the improvement of the adsorption ability of phosphate-imprinted SiO2 microspheres. With the increase in the initial phosphate concentration, the adsorption capacity of hybrid particles to phosphate ions increased to 274 mg/g at pH = 7 and 15 °C. The acid condition and the temperature below the low critical solution temperature (LCST) of PNIPAM are favorable to the adsorption of phosphate ions by PNIPAM/SiO2 hybrid particles, and the maximum adsorption capacity can reach 287 mg/g (at pH = 5 and 15 °C). The phosphate imprinted polymer/inorganic hybrid material is expected to be put to use in the fields of phosphate ions adsorption, separation, and recovery.