In the present investigation, a procedure was developed to recover VF800AT steel stamping punches by the GMAW process, using Tube-Alloy 260-G, a gas-shielded, metal-cored wire that deposits a martensitic alloy steel. The samples were pre-heated at 450, 500 and 550 °C, and after weld repaired, were submitted to tempering. The samples were characterized before and after the weld repair concerning the macrostructure, microstructure, and microhardness. The correlation of the hardness in the weld metal, heat affected zone and base metal regions with the heat treatments was evaluated statistically by analysis of variance. To experimentally validate this condition, a performance test of the new and weld repaired punches was carried out. Optical microscopy, roughness measurements, and scanning electron microscopy were carried out to evaluate the geometric shape of the radius of the cutting-edge radius and the type of wear acting on the punches. Punches pre-heated to 450 °C and submitted to one tempering step presented the best results, being the most suitable to recover stamping tools made of VF800AT steel by the GMAW process.
Medium-carbon steels are susceptible to heat-affected zone (HAZ) hardening during welding. This study evaluated the effects of preheating temperature and joint geometry on mechanized gas metal arc welded (GMAW) joints in 6.3 mm thick SAE 1045 steel. Butt and fillet joints were welded under conventional single-pass conditions from room temperature to 250 °C, while an additional two-pass procedure was evaluated separately. Metallography and hardness were evaluated for both joint geometries, whereas tensile and Charpy V-notch tests were performed only on butt joints. Significant joint geometry × preheating condition interactions were identified for weld metal (WM) area, HAZ area, WM hardness and HAZ hardness. Average HAZ hardness remained below 300 HV10 for all conventional single-pass conditions. Among the butt joint single-pass conditions, no statistically significant effect of preheating was detected for ultimate tensile strength (UTS) or Charpy absorbed energy, and all tensile specimens fractured in the base metal (BM). The two-pass procedure was treated descriptively because the second deposition simultaneously altered multiple welding variables. Overall, the effects of preheating on WM and HAZ areas and hardness were joint-geometry-dependent under the investigated conditions.