This study investigated the adsorption capacities and photocatalytic activities of geopolymer-zeolite composite materials by incorporating different amounts of zeolite and TiO2 in a geopolymer matrix for dye removal. Geopolymers with SiO2/Al2O3 molar ratio of 2.5 were synthesized from metakaolin. The geopolymers containing zeolite and TiO2-doped zeolite exhibited similar behavior in terms of mineral compositions, microstructures and chemical frameworks. The compressive strength of geopolymer-zeolite composite materials decreased with increasing amount of zeolite and TiO2-doped zeolite (0–40 wt%) because of the increase in the porosity of composite materials. The maximum methylene blue adsorption capacity and photocatalytic efficiency of the powdered geopolymer composites with 40 wt% TiO2-doped zeolite was 99.1% and was higher than that of the composites with 40 wt% zeolite without TiO2-doping (92.5%). In addition, the geopolymer composites with TiO2-doped zeolite exhibited excellent stability after repeated usage as photocatalysts. The adsorption capacity and photocatalytic activity of pelletized geopolymer composites decreased because of the reduction in their specific surface area.
26 April 2010 in Waste Management & Research: The Journal for a Sustainable Circular Economy
Synthesis of zeolites from combustion by-products, including fly ash, bottom ash and rice husk ash, was studied. A molar ratio of SiO2/Al2O3 of 1.5 was used for the syntheses. Refluxing and hydrothermal methods were also used for synthesis for comparison. The reaction temperatures of refluxing and hydrothermal methods were 100°C and 130°C, respectively. Sodalite, phillipsite-K, and zeolite P1 with analcime were obtained when fly ash, bottom ash and rice husk ash were used as starting materials, respectively. With rice husk ash as a starting material, zeolite P1 was produced. This result had advantages over previous studies as there was no prior activation required for the synthesis. The concentrations and types of alkaline used in the synthesis also determined the zeolite type. The different zeolites obtained from three systems were measured for specific surface area and pore size by using BET and Hg-porosimetry, respectively. Ammonium exchange capacities of the synthesised powders containing zeolites, sodalite, zeolite P1 and phillipsite-K were 38.5, 65.0 and 154.7 meq 100 g -1, respectively.
Metakaolin based geopolymer binder was synthesized using variable factors such as Na2O/SiO2, Na2O/Al2O3 and H2O/Na2O molar ratios as well as curing time. Metakaolin was used as an alumino silicate source incorporating with strong alkali activators; sodium hydroxide solution to undergo polycondenation and hence a formation of hardened geopolymeric binder. This work was aimed to investigate the effect of Na2O/SiO2, Na2O/Al2O3 and H2O/Na2O ratios, as well as curing time on phase transformation. The chemical composition, phase development and microstructure of reaction products were examined by X-ray fluorescence, X-ray diffraction analysis and scanning electron microscopy with respect to their final compressive strength. Increasing the molar ratios of Na2O/Al2O3 and H2O/Na2O tended to favour the transformation of amorphous gel to various types of crystalline zeolite. Sodalite (pseudo-phase zeolite) and zeolite belonging to the Faujasite group, as well as zeolite X and A were identified in these mixtures. Based on this study, systems that favoured the formation of zeolitic products tended to possess lower strengths.
26 November 2024 in Construction and Building Materials
Faujasite and analcime were synthesized by two-step process via hydrothermal method using the rice husk ash and metakaolin as starting materials. In the first step, the raw materials were prepared using the SiO2/Al2O3molar ratio of 4 and pretreatment with NaOH solution under various stirring conditions. The suspension was subjected to hydrothermal treatment at various reacting time and temperature in second step. The mineralogy, morphology, specific surface area and cation exchange capacity of the synthesized products were investigated using X-ray diffraction, Scanning electron microscopy, N2adsorption and desorption isotherm and ammonium acetate method, respectively. Faujasite was obtained using low temperature and short-time synthesis, while the analcime was obtained at high temperature and long-time synthesis. The stirring time did not affect zeolite types but the specific surface area. The cation exchange capacity of the synthetic faujasite and analcime were 263-280 and 280-302 meq/100 g, respectively.
This paper discusses the effects of the silicon dioxide to aluminium oxide molar ratio, sodium oxide to aluminium oxide molar ratio and concentration of sodium hydroxide on the water absorption and compressive strength of synthesised fly ash-based geopolymers. Geopolymer pastes were prepared using fly ash mixed with an alkaline activator consisting of sodium hydroxide solution and sodium silicate solution. The phase composition, microstructure and chemical bonding of the synthesised products were characterised after 7 and 28 days using X-ray diffraction, scanning electron microscopy and Fourier-transform infrared spectroscopy, respectively. The synthesised geopolymer with a silicon dioxide to aluminium oxide molar ratio of 5 and a sodium oxide to aluminium oxide molar ratio of 1.2, activated with 10 M sodium hydroxide, was found to have the highest strength and the lowest water absorption. The compressive strength was observed to increase with increasing silicon dioxide to aluminium oxide molar ratio. A high initial molar ratio of sodium oxide to aluminium oxide enhances the water absorption and decreases the strength of the geopolymer sample. The dissolution of silica and alumina from the starting materials becomes more efficient as the concentration of sodium hydroxide increases.