Lithium‐ion batteries (LIBs) have flourished in power and energy storage, followed by the waste batteries that are pouring into the market. For waste graphite anode, how to deal with high efficiency, high economic efficiency, and low environmental pollution has become a huge challenge. In the work, a deep eutectic solvent (DES), with a low melting point, low cost, and natural environmental protection, is applied as a green reagent to realize the sustainable and direct upcycling of waste graphite. Substances in DES existing in the form of ions and charged P‐containing groups are more likely to attack defect‐rich graphite and realize in situ phosphorus doping, and doped phosphorus participates in the construction of Li 3 PO 4 ‐rich solid electrolyte interphase (SEI). Due to the reconstruction of phosphate‐rich interfacial film, the capacity of regenerated graphite maintains as high as 365 mAh g −1 at 0.5C with a capacity retention rate of 95.5%, which is much higher than that of waste graphite and even commercial graphite. In addition, the low melting point of DES makes the regeneration temperature significantly lower, so that the strategy reduces the CO 2 emissions of energy consumption. More importantly, the environment and economy have been optimized, which is conducive to its large‐scale promotion in industry.
Developing efficient heterojunction photocatalysts is essential to address the challenge of degrading persistent organic pollutants. In this study, a multi-scale characterization strategy was employed to investigate the implications of interfacial connectivity between synthesized graphitic carbon nitride (g-C3N4) /bismuth oxychloride (BiOCl)e removal of Rhodamine B (RhB) and Methyl Orange (MO). Morpho-structural characterizations, including Scanning/Transmission Electron Microscopy (SEM/TEM), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), and N2 physisorption (Brunauer–Emmett–Teller (BET)) analyses, confirmed the successful construction of an intimate interfacial contact between g-C3N4 and BiOCl. The optimized composite (15% g-C3N4/BiOCl), prepared via a one-step hydrothermal method, exhibited enhanced photocatalytic performance following pseudo-first-order kinetics described by the Langmuir–Hinshelwood model, with apparent rate constants of 0.166 min−1 for MO and 0.519 min−1 for RhB. Under visible-light irradiation, degradation efficiencies of 98% for MO (120 min) and 99% for RhB (35 min) were achieved, outperforming the pristine components. Complementary optical and electrochemical analyses indicate improved light absorption and charge-separation efficiency in the heterojunction system. In addition, the photocatalyst demonstrated good operational stability over four consecutive cycles, maintaining 91.70% activity for MO and 99.76% for RhB. Overall, this work highlights the synergistic photocatalytic g-C3N4/BiOCl heterojunction and provides a valuable insight to guide the design of advanced materials for pollutant remediation.
NASICON-type Na3V2(PO4)3 (NVP) is widely regarded as a promising cathode for sodium-ion batteries owing to its robust three-dimensional framework and high operating voltage (~3.4 V vs. Na+/Na). However, NVP suffers severe capacity degradation under fast-charging conditions due to its intrinsically low electronic conductivity, which critically impedes its practical deployment. Herein, we systematically investigate the fast-charging failure mechanism of NVP and propose a trace Sm3+ doping strategy (x = 0.03) to address this limitation. Undoped NVP retains only 13.5% and 56.62% of its initial capacity after 1000 cycles at 5000 mA g−1 and 1307 cycles at 2000 mA g−1, respectively. Post-cycling scanning electron microscopy (SEM) reveals extensive crack formation and particle pulverization, providing direct morphological evidence for structural failure. To overcome this, Sm3+-doped Na3V1.97Sm0.03(PO4)3/C (NVPSM) is synthesized via a sol–gel method. X-ray diffraction (XRD) confirms that the NASICON phase is preserved. Raman spectroscopy reveals an improved graphitization degree (ID/IG = 0.97 vs. 1.02 for NVP), and X-ray photoelectron spectroscopy (XPS) verifies the V3+ oxidation state and the incorporation of Sm3+. Electrochemically, NVPSM achieves capacity retentions of 60.3% after 2300 cycles at 5000 mA g−1 and 83.89% after 1436 cycles at 2000 mA g−1. Electrochemical impedance spectroscopy confirms reduced charge-transfer resistance, and post-cycling SEM shows markedly improved structural integrity. These results demonstrate that trace rare-earth doping effectively mitigates fast-charging-induced structural failure in NVP-based cathodes.
Researchers on degraded lithium ion batteries are increasingly focusing on direct recycling, a more sustainable approach than pyrometallurgy and hydrometallurgy. More precisely, the upcycling approach has attracted widespread attention. However, beyond economic advantages, the sustainability of these upcycling strategies, including their environmental footprint and long‐term viability, is equally critical for achieving truly circular battery systems. This review first provides a multi‐level, multi‐scale overview of the degradation mechanisms of polycrystalline cathodes and the advantages of single‐crystal cathodes. It then focuses on strategies for regenerating single‐crystal cathodes, covering solid‐state sintering, and molten‐salt‐assisted and hybrid‐assisted upcycling strategies. Additionally, the review explores the advantages of single‐crystal cathodes and strategies for optimizing their single‐crystallization from the perspectives of surface modification, structural optimization, defect engineering, kinetics, and environmental impact. Finally, this article highlights the significant competitive edge of single‐crystal cathodes in lithium‐ion battery recycling and proposes the following: (i) classify and grade degraded cathodes prior to recycling; (ii) establish a database for degraded cathodes and apply machine learning; (iii) develop nickel‐rich, cobalt‐poor single‐crystal cathodes; and (iv) quantify the carbon and water footprints during the recycling process.
Layered cathodes (LiNixCoyMnzO2, NCM) have emerged as critical materials for batteries and energy storage fields by virtue of their high energy density. However, NCM materials undergo rapid performance degradation and severe capacity fading under harsh conditions of long-term cycling and high voltage. Currently, research regarding spent NCM materials mainly concentrates on failure analysis and modification processes at the macroscopic scale. Nevertheless, the failure mechanisms of NCM, the intrinsic processes during repair and modification, and the fundamental origins of performance improvement are generally embedded in structural evolution at the nanoscale or even atomic scale. This review first discusses the failure mechanisms of NCM. Particularly, the main content focuses on lattice distortion and layered structural instability at the lattice level, migration of nanoscale species together with performance degradation induced by side reactions at the interface level, and generation of nanocracks at the particle level. Moreover, this paper reviews the characterization methods applied at the nanometer scale, and two modification strategies are summarized, namely nanoscale coating and elemental doping. It is expected to provide theoretical references and technical insights for constructing efficient and controllable targeted modification strategies of layered NCM cathodes and developing high-performance ternary cathode materials.