Two novel cycloalkoxy silane compounds (ED1 and ED2) were synthesized and used as the external electron donors (EEDs) in Ziegler–Natta catalysts with diethyl 2,3-diisopropylsuccinate as internal electron donor. The results indicated that the Ziegler–Natta catalysts using ED1 and ED2 as EEDs had high catalytic activities and good stereoselectivities. The melt flow rate (MFR) and gel permeation chromatography (GPC) results revealed that the obtained polypropylene has higher MFR and lower average molecular weights than the commercial EED cyclohexyl methyl dimethoxysilane. The differential scanning calorimetry (DSC) results indicated that new isospecific active centers formed after the introduction of new external donors. The work implied that the novel EEDs could improve the hydrogen sensitivities of the catalyst system and obtain polymers with high melt flow rate.
A series of N-acetyl-O-(ω-alkenyl)-l-tyrosine ethyl esters were synthesized by the reaction of vinyl bromides (4-bromo-1-butene, 6-bromo-1-hexene, 8-bromo-1-octene and 10-bromo-1-decene) with N-acetyl-l-tyrosine ethyl ester. 1H NMR, elemental analysis, FT-IR, and mass spectra were performed for these N-acetyl-O-(ω-alkenyl)-l-tyrosine ethyl esters. The novel titanium complex can catalyze the copolymerization of ethylene and N-acetyl-O-(ω-alkenyl)-l-tyrosine ethyl esters efficiently and the highest catalytic activity was up to 6.86 × 104 gP·(molTi)−1·h−1. The structures and properties of the obtained copolymers were characterized by FT-IR, (1H)13C NMR, GPC, DSC, and water contact angle. The results indicated that the obtained copolymers had a uniformly high average molecular weight of 2.85 × 105 g·mol−1 and a high incorporation ratio of N-acetyl-O-(but-3-enyl)-l-tyrosine ethyl ester of 2.65 mol % within the copolymer chain. The units of the comonomer were isolated within the copolymer chains. The insertion of the polar comonomer into a copolymer chain can effectively improve the hydrophilicity of a copolymer.
Impact polypropylene copolymers (ICPs) are promising thermoplastics for recyclable high-voltage direct-current (HVDC) cable insulation, yet the links among molecular sequence, crystalline framework, multiphase topology, and charge transport remain unclear. A homopolymer-matrix (HICP), a random-copolymer-matrix (RICP), and a commercial high-phase-continuity (CICP) ICP were compared across molecular, crystalline, morphological, rheological, electrical, and mechanical scales. Relative to HICP, matrix randomization in RICP raised the soluble fraction at ≤35 °C from 18.92 to 27.21 wt%, lowered crystallinity from 51.1% to 32.1%, and reduced the effective crystalline-layer contribution from 7.84 to 4.05 nm. Concurrently, the characteristic trap depth increased from 0.92 to 1.05 eV, the maximum local space-charge density decreased from 65.5 to approximately 28.4 C m−3, and the characteristic DC breakdown strength rose from 226.2 to 310.8 kV mm−1, while the tensile modulus fell from 1000 to 612 MPa. CICP combined the lowest modulus (89.4 MPa, without fracture at the 630% instrument limit) with the lowest space-charge density (below 12.5 C m−3) and the highest breakdown strength (384.4 kV mm−1). Matrix-sequence regulation and multiphase topology thus provide a structural route to reconcile flexibility with high-field stability in recyclable PP cable insulation.
Softening impact-resistant polypropylene (PP) copolymers (ICPs) may be accompanied by reduced breakdown performance; coordinating mechanical and electrical properties is closely related to crystalline-framework and rubber-rich-phase organization. Homopolymer PP matrix HICP and random copolymer PP matrix RICP formed the primary comparison, with high-phase-continuity CICP as a reference, through composition, fractionation, crystalline structure, morphology, viscoelasticity, and charge analyses. Relative to HICP, RICP matrix randomization extended crystallizability distributions toward lower temperatures, refined the crystalline framework, and expanded interphase regions. Tensile and flexural moduli decreased by 38.8% and 38.7%, respectively, while Weibull characteristic breakdown strength increased from 226.2 to 310.8 kV/mm. CICP, containing 23.3 wt% ethylene, comprised a continuous low-crystallinity/rubber-rich phase with dispersed PP crystalline domains. Its tensile modulus was 89.4 ± 4.9 MPa; it retained partial break in notched impact testing at −20 °C and a characteristic breakdown strength of 384.4 kV/mm. Thermally stimulated depolarization current, conduction, and space-charge results indicated that local trapping environments and multiphase transport pathways jointly regulate charge migration and accumulation, providing a charge-behavior basis for maintaining high insulation performance as flexibility increases. The relationships linking molecular sequences, crystalline organization, phase connectivity, and mechanical–electrical responses provide a basis for designing multiphase PP-based DC cable insulation.