Hydroxyapatite (HA)-coated metals are biocompatible composites, which have potential for various applications for bone replacement and regeneration in the human body. In this study, we proposed the design of biocompatible, flexible composite implants by using a metal mesh as substrate and HA coating as bone regenerative stimulant derived from a simple sol–gel method. Experiments were performed to understand the effect of coating method (dip-coating and drop casting), substrate material (titanium and stainless steel) and substrate mesh characteristics (mesh size, weave pattern) on implant’s performance. HA-coated samples were characterized by X-ray diffractometer, transmission electron microscope, field-emission scanning electron microscope, nanoindenter, polarization and electrochemical impedance spectroscopy, and biocompatibility test. Pure or biphasic nanorod HA coating was obtained on mesh substrates with thicknesses varying from 4.0 to 7.9 μm. Different coating procedures and number of layers did not affect crystal structure, shape, or most intense plane reflections of the HA coating. Moduli of elasticity below 18.5 GPa were reported for HA-coated samples, falling within the range of natural skull bone. Coated samples led to at least 90% cell viability and up to 99.5% extracellular matrix coverage into a 3-dimensional network (16.4% to 76.5% higher than bare substrates). Fluorescent imaging showed no antagonistic effect of the coatings on osteogenic differentiation. Finer mesh size enhanced coating coverage and adhesion, but a low number of HA layers was preferable to maintain open mesh areas promoting extracellular matrix formation. Finally, electrochemical behavior studies revealed that, although corrosion protection for HA-coated samples was generally higher than bare samples, galvanic corrosion occurred on some samples. Overall, the results indicated that while HA-coated titanium grade 1 showed the best performance as a potential implant, HA-coated stainless steel 316 with the finest mesh size constitutes an adequate, lower cost alternative.
The application of frontal polymerization to additive manufacturing has advantages in energy consumption and speed of printing. Additionally, with frontal polymerization, it is possible to print free-standing structures that require no supports. A resin was developed using a mixture of epoxies and vinyl ether with an iodonium salt and peroxide initiating system that frontally polymerizes through radical-induced cationic frontal polymerization. The formulation, which was optimized for reactivity, physical properties, and rheology, allowed the printing of free-standing structures. Increasing ratios of vinyl ether and reactive cycloaliphatic epoxide were found to increase the front velocity. Addition of carbon nanofibers increased the front velocity more than the addition of milled carbon fibers. The resin filled with carbon nanofibers and fumed silica exhibited shear-thinning behavior and was suitable for extrusion-based printing at a weight fraction of 4 wt %. A desktop 3D printer was modified to control resin extrusion and deposition with a digital syringe dispenser. Flexural properties of molded and 3D-printed specimens showed that specimens printed in the transverse direction exhibited the lowest strength, likely due to the presence of voids, adhesion issues between filaments, and preferential carbon nanofiber alignment along the filaments. Finally, free-standing printing of single, angled filaments and helical geometries was successfully demonstrated by coordinating ultraviolet-based reaction initiation, low air pressure for resin extrusion, and printing speed to match front velocity.
This manuscript explores the disassembly potential of ultrasonically welded thermoplastic composite joints for reuse or recycling through resistance heating via a nanocomposite film located at the welded interface. Nanocomposite films containing multi-walled carbon nanotubes (MWCNTs) were characterized for thermo-electrical behavior to assess self-heating. It was generally observed that maximum temperature increased with MWCNT and film thickness. To demonstrate potential for disassembly, glass fiber/polypropylene adherends were welded with nanocomposite films. Shear stress during disassembly was measured for three initial adherend’s surface temperatures. It was found that the required tensile load decreased by over 90% at the highest temperatures, effectively demonstrating the potential for disassembly via electrically conductive films. Fracture surfaces suggested that disassembly was facilitated through a combination of nanocomposite and matrix melting and weakened fiber–matrix interface. Limitations, such as slow heating rates and the loss of contact at the interface, imply that the method could be more suited for recycling, instead of repair and reuse, as the heat-affected zone extended through the adherends’ thickness at the overlap during heating.