Stable aqueous iron oxide nanoparticle dispersions were prepared by coprecipitation of ferrous (Fe2+) and ferric (Fe3+) aqueous solution by a base in the presence of graft copolymers, poly(glycerol monoacrylate)-g-poly(PEG methyl ether acrylate) (PGA-g-PEG). PGA-g-PEG was prepared by acidic hydrolysis of poly(solktal acrylate)-g-poly(PEG methyl ether acrylate), which was synthesized by copolymerization of solktal acrylate and PEG methyl ether acrylate by atom transfer radical polymerization (ATRP). The size of the magnetite nanoparticles can be controlled from 4 nm to 18 nm by varying the graft density of the graft copolymers. Structural characterization using X-ray diffraction showed the presence of only the magnetite phase in the nanoparticles. Thermogravimetric analysis confirmed the presence of the graft copolymers on the magnetite surface. The magnetic characterization of the nanoparticles showed that they were superparamagnetic at room temperature.
Highly stable aqueous magnetic fluids were prepared by coating Fe3O4 nanoparticles with poly(glycerol monoacrylate), poly(glycerol monomethacrylate), or diblock copolymers, poly(acrylic acid)-b-poly(glycerol monoacrylate), poly[(N,N-dimethylamino)ethyl methacrylate]-b-poly(glycerol monomethacrylate) or poly(ethylene glycol) monomethyl ether-b-poly(glycerol monoacrylate). These homopolymers and block copolymers were synthesized by atom transfer radical polymerization. These dispersions were stable in 10% NaCl, 10% CaCl2, or in wide pH ranges. In these magnetic fluids, poly(glycerol monoacrylate) or poly(glycerol monomethacrylate) were chemisorbed onto the Fe3O4 nanoparticle surface through their 1,2-diol groups by forming five-membered chelate rings with the Fe atoms, while the other blocks in the cases of the block copolymers as the stabilizers extended into the water matrix. Thus the nanoparticles prepared with these three block copolymers mentioned above respectively contain negatively charged, positively charged or uncharged and biocompatible surfaces under physiological conditions. This procedure provided a good choice for preparing stable magnetic fluids with tailored surfaces and/or tailored functional groups on the surfaces of the magnetic nanoparticles.
Nanocarriers with multilayer core–shell architecture were prepared by coating a superparamagnetic Fe3O4 core with a triblock copolymer. The first block of the copolymer formed the biocompatible outermost shell of the nanocarrier. The second block that contains amino groups and hydrophobic moiety formed the inner shell. The third block bound tightly onto the Fe3O4 core. Chlorambucil (an anticancer agent) and indomethacin (an anti-inflammation agent), each containing a carboxyl group and a hydrophobic moiety, were loaded into the amino-group-containing inner shell by a combination of ionic and hydrophobic interactions. The release rate of the loaded drugs was slow at pH 7.4, mimicking the blood environment, whereas the release rate increased significantly at acidic pH, mimicking the intracellular conditions in the endosome/lysosome. This can be attributed to the disruption of the ionic bond caused by protonation of the carboxylate anion of the drugs and the swelling of the inner shell caused by protonation of the amino groups.
2 November 2006 in Journal of Biomedical Materials Research Part A