Future generations of wearable electronic systems and mobile communication place a great demand for harvesting energy from ambient environments or human movements. Soft fiber-based electric power generators are attractive in meeting the requirements of wearable devices because of efficient energy conversion performance, high durability and comfort. In this paper, we present a novel all-fiber wearable electric power nanogenerator, which consists of a PVDF–NaNbO3 nanofiber nonwoven fabric as an active piezoelectric component, and an elastic conducting knitted fabric, made from segmented polyurethane and silver coated polyamide multifilament yarns, as the top and bottom electrodes. The non-uniform deformation distribution in a compressed nanogenerator device determines the complex operating modes in the piezoelectric nanofiber nonwoven fabric. The nanogenerator consistently produces a peak open-circuit voltage of 3.4 V and a peak current of 4.4 μA in cyclic compression tests at 1 Hz and a maximum pressure of 0.2 MPa, which is comparable to normal human walking motion. More importantly, the all-fiber nanogenerator retains its performance after 1 000 000 compression cycles, demonstrating great promise as a wearable energy harvester that converts the mechanical energy of human movement into electricity.
The use of lead-free materials has recently become a very important issue in environmental protection of the earth. Two groups of lead-free ceramics, based (KNN) and based (BNKT), were studied for their thermal, dielectric, and pyroelectric properties as candidates for pyroelectric sensor applications. The BNKT-based ceramic, (BNKLBT), shows excellent pyroelectric properties when compared with KNN-based ceramic and lead zirconate titanate. Its properties were measured as follows: pyroelectric coefficient , pyroelectric figure of merit of current, voltage, and detectivity , , and . With these outstanding pyroelectric properties, the BNKLBT ceramic can be a promising material for pyroelectric sensor applications. The BNKLBT ceramic with different thicknesses (i.e., 0.3, 0.5, and ) have been used as the sensing element for fabricating infrared detectors. The current responsivity of the sensors was evaluated as functions of frequency.
Thermal tuning of phononic bandgaps in megahertz range was demonstrated in ferroelectric ceramic-based phononic crystal structure. Temperature variation across ferroelectric phase transition, accompanied by substantial changes in acoustic velocities, leads to a shift in the phononic bandstructure of a two-dimensional (Ba,Sr)TiO3/epoxy composite sample over a range of 10 °C. Experimental results are supported by modelings based on plane-wave expansion calculations. The high tunability of phononic bandstructure is advantageous for active control of ultrasound transmissions.
1 October 2008 in Journal of the American Ceramic Society
Doping effects with respect to the electrical properties of morphotropic phase boundary (Bi0.5Na0.5)0.94Ba0.06TiO3 thin films epitaxially grown on CaRuO3 electroded (LaAlO3)0.3(Sr2AlTaO6)0.35 (001) substrates were investigated. Substantial enhancement of ferroelectricity and piezoelectricity has been achieved in La+Ce codoped films with a remanent polarization Pr of 29.5 μC/cm2 and a remanent piezoelectric coefficient d33,f of 31 pm/V, whereas Mn doping seems more favorite to reduce the leakage current by two order of magnitude. Both doped films exhibited diodelike I-V characteristics, which are correlated with resistance switching effect.
( 0.95 − x ) ( Bi 1 ∕ 2 Na 1 ∕ 2 ) TiO 3 – x ( Bi 1 ∕ 2 K 1 ∕ 2 ) TiO 3 – 0.05 BaTiO 3 lead-free piezoelectric ceramics (abbreviated as BNT–BKT–BT100x with x varying from 0 to 20 mol %) are prepared by a solid-state reaction process. Variation of the dielectric properties and microstructure of BNT–BKT–BT100x ceramics with BKT content is studied. The results indicate that the relative permittivity εr and loss tangent tanδ vary with the BKT amount. Scanning electron microscope observation also indicates that BKT in high amount affects the microstructure. X-ray diffraction analysis shows that the incorporated BKT diffuses into the BNT–BT lattice to form a solid solution during sintering.