Jidong Ma

Dr. Jidong Ma


Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 November 2018 in Materials
Verified
Journal Article
Open access
PDF file
SGSiyong Gu
Siyong Gu
MQMingli Qin
Mingli Qin
HZHouan Zhang
Houan Zhang
JMJidong Ma
Jidong Ma
This work reports the preparation of La2O3 uniformly doped Mo nanopowders with the particle sizes of 40–70 nm by solution combustion synthesis and subsequent hydrogen reduction (SCSHR). To reach this aim, the foam-like MoO2 precursors (20–40 nm in size) with different amounts of La2O3 were first synthesized by a solution combustion synthesis method. Next, these precursors were used to prepare La2O3 doped Mo nanopowders through hydrogen reduction. Thus, the content of La2O3 used for doping can be accurately controlled via the SCSHR route to obtain the desired loading degree. The successful doping of La2O3 into Mo nanopowders with uniform distribution were proved by X-ray photon spectroscopy and transmission electron microscopy. The preservation of the original morphology and size of the MoO2 precursor by the La2O3 doped Mo nanopowders was attributed to the pseudomorphic transport mechanism occurring at 600 °C. As shown by X-ray diffraction, the formation of Mo2C impurity, which usually occurs in the direct H2 reduction process, can be avoided by using the Ar calcination-H2 reduction process, when residual carbon is removed by the carbothermal reaction during Ar calcination at 500 °C.

29 January 2018 in International Journal of Materials Research
Verified
Journal Article
Closed access
JMJidong Ma
Jidong Ma
MQMingli Qin
Mingli Qin
XDXiangying Ding
Xiangying Ding
DKDil Faraz Khan
Dil Faraz Khan
HZHouan Zhang
Houan Zhang
Fe–Co-based soft magnetic alloys with excellent magnetic properties were prepared by metal injection moulding and hot isostatic pressing. The effect of processing parameters on microstructure and magnetic properties of the alloy were investigated. Good magnetic performance of Fe-50 %Co alloy with a maximum permeability of 9550, saturation induction of 2.42 T, and coercive force of 68.14 A m–1 was achieved. Hot isostatic pressing processing resulted in a near-full density and the achieved saturation induction exceeded the reported value (1.99 to 2.26 T) of Fe-50 %Co produced by metal injection moulding.

10 December 2019 in International Journal of Materials Research
Verified
Journal Article
Closed access
JMJidong Ma
Jidong Ma
HZHouan Zhang
Houan Zhang
LYLiang Yang
Liang Yang
DKDil Faraz Khan
Dil Faraz Khan
YYYihang Yang
Yihang Yang
XZXiaofeng Zhang
Xiaofeng Zhang
Fe-0.8% P soft magnetic alloy was prepared by powder metallurgy. The compressibility and purity of powder were improved through collocation of powder particles and annealing treatment. The effect of sintering temperature on density, microstructure, and magnetic properties of the alloys was studied. Results show that the magnetic performance of the alloy was enhanced due to increased density because of the formation of liquid phase at low temperature and δ phase at high temperature. The optimum magnetic properties of Fe-0.8% P alloy with magnetic induction (B6000) of 1.83 T, maximum permeability of 18706 and coercive force of 30 A m−1 were obtained due to increased density (relative density 99.4%) and sintering temperatures.