In this study, Multiwalled carbon nanotubes (MWCNTs) were oxidized by a mixture of sulfuric acid and nitric acid (V:V = 3:1) at 70 °C for 1, 2, and 4 h, respectively. The oxidized MWCNTs were characterized by N2 adsorption, Fourier-transform infrared spectroscopy (FT-IR), X-ray photoelectron spectroscopy (XPS), thermal gravimetric analysis (TGA), and Raman spectroscopy to determine the oxidation degree. The dispersion of the MWCNTs was investigated by UV-vis-NIR, SEM, and dynamic light scattering measurements. Results show that sulfonitric treatment increased the surface area and total pore volume and reduced the average pore diameter of MWCNTs. The treatment promoted the formation of oxidized species on the surface MWCNTs, as identified by FT-IR, TGA, and X-ray photoelectron spectroscopy measurements, and more oxygen-containing functional groups were generated when treatment time was extended. Moreover, a general relationship between oxidation degree and dispersibility of MWCNTs in water was established. UV-vis-NIR and dynamic light scattering measurements and SEM images revealed that MWCNTs with higher oxidation degree showed better dispersibility in water.
Sulphoaluminate cement has the advantage of low-temperature application performance, but its hydration mechanism at low temperatures is not yet clear. Anhydrous calcium sulfoaluminate (C4A3S) is the main mineral in the composition of sulfoaluminate cement clinkers. In this paper, C4A3S mixed with gypsum (CaSO4∙2H2O) to form a C4A3S-CSH2 cement system; X-ray diffraction (XRD), thermogravimetric analysis (TG-DTG), scanning electron microscopy (SEM) and mercury intrusion analysis (MIP) to clarify the effect of temperatures on the hydration properties of C4A3S-CSH2 cement system. The results showed that hydration of the C4A3S-CSH2 cement system could carry on at low temperatures, even at −15 °C. The main hydration product was ettringite. Low temperatures did not change the types of the hydration products, but the low temperature of 0 °C was more favorable for the formation of ettringite. The early hydration of the C4A3S-CSH2 cement system was inhibited by the decrease in temperature. However, hydration of the cement at 0 °C continued at a high rate after one day. Morphologies of the ettringite for the C4A3S-CSH2 cement system at −15 °C were needle-like structures, while they were of columnar structure at 0 °C. The compressive strength of samples at 0 °C reached 82 MPa, which is significantly higher than that at 20 °C.
Air quenched slag is processed by a fast air cooling method which is developed with the advantages of recovering heat from molten slag and water conservation compared to the water quenching method. Air quenched slags with different chemical compositions are synthesized in the lab by designing three chemical composition ratios: (CaO + MgO)/(SiO2 + Al2O3), CaO/MgO and SiO2/Al2O3, which are donated as CM/SA, C/M and S/A, respectively. The effect of different chemical compositions on the phase compositions of synthetic air quenched slag, the strength and hydration properties of slag blends were investigated by using various characterization techniques. The results show that the amorphous content of air quenched slag decreased with the increasing basicity CM/SA of slag. The S/A ratio of slag was the dominant factor for the compressive strength of slag blends at 28 days and negatively correlated with strength. Decreasing the S/A ratio of slag increased the reactivity of slag and its reaction degree indicated by higher hydration heat release, lower CH content, greater chemical combined water amount and denser microstructure. Moreover, thermodynamic modelling revealed that a higher S/A of slag leads to the increase of C-(A)-S-H and AFt contents, whilst decreasing the amounts of Ht, AFm-SO4 phases and the total volume of hydrates.
In order to improve the properties of lime-based mortars and promote the green development of the construction industry, blended lime-based mortars were prepared by using carbide slag instead of hydrated lime, and the additions of Portland cement and sulphoaluminate cement were studied in our work. The paper focused on mechanical properties, porosity, capillary water absorption and drying shrinkage of both types of blended mortars. The chemical composition and microstructure of hydration products were investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results show that sulphoaluminate cement provided more contributions to mechanical properties, capillary water absorption and early shrinkage compared to Portland cement.