The advent of high-entropy alloys (HEAs) provides new possibilities for the metallurgical community. CoCrFeNi-based alloys have been widely recognized to demonstrate superior mechanical properties, amongst the high-entropy alloy systems; in particular, they possess an outstanding tensile ductility and work-hardening capacity. Additive manufacturing (AM) uses a layer-by-layer material deposition approach to build parts directly from computer-aided design models, which are capable of producing near-net-shape HEAs with superior mechanical properties, surpassing traditional manufacturing methods that require a time-consuming post-treatment process, such as cutting, milling, and molding. Moreover, the rapid solidification inherent in AM processes induces the formation of high-density dislocations, which are capable of enhancing the mechanical properties of HEAs. This review comprehensively investigates and summarizes the diverse strengthening mechanisms within CoCrFeNi-based alloys produced using AM technologies, with a specific focus on their influence on tensile properties. A correlation is established between the AM processing parameters and the resultant phases and microstructures, as well as the mechanical properties of CoCrFeNi-based HEAs, which provide guidelines to achieve a superior strength–ductility synergy.
Laser powder bed fusion (L-PBF) of near-β titanium alloys typically produces coarse columnar grains and strong textures, which induce anisotropic mechanical behavior. Here, 5 wt.% tantalum (Ta) particles were doped into Ti-5Al-5Mo-5V-3Cr (Ti-5553) powder to concurrently inhibit microstructural anisotropy and contribute to enhanced strength–ductility synergy via solidification modification. During the L-PBF process, unmelted Ta particles provided heterogeneous nucleation sites, while dissolved Ta generated local constitutional undercooling. Together, these effects reduced the average β-grain size from 47.23 ± 27.5 to 12.28 ± 11.8 μm and weakened the texture, as well as increased yield strength from 870 to 990 MPa while retaining 28% elongation. After solution treatment and aging, Ti-5553-Ta reached a yield strength of 1196 MPa and 16.0% elongation. Local Ta-enriched precipitate-free zones and refined α precipitates contributed to the improved post-treatment ductility.