The rigid coupling between the emitted THz polarization and the magnetization orientation of a spintronic emitter enables polarization control, but conventional approaches require tuning an external magnetic field. Here, we demonstrate that in an ultrathin W/FeGa/Pt heterostructure deposited on a PMN-PT (011) substrate, the polarization plane can be smoothly rotated by 40° using a DC voltage alone, under a fixed, weak bias magnetic field (24 Oe). The key element is a 5-nm-thick Galfenol (FeGa) layer sandwiched between heavy metals with opposite signs of the spin Hall angle: it simultaneously serves as the source of the ultrafast spin current and as a magnetostrictive transducer that converts substrate strain into a magnetic response. THz spintronic magnetometry, which probes the structure under the actual conditions of THz generation, allows us to quantitatively correlate the polarization rotation angle with the strain-induced magnetoelastic anisotropy transferred to the film. The obtained results are directed toward the design of compact THz sources with electrically tunable polarization.
We investigate terahertz (THz) emission mechanisms in spintronic emitters – Co (3 nm), graphene (Gr)/Co (3 nm), and Co (3 nm)/FeMn (5 nm) – grown on quartz substrates. Magnetic properties were characterized in the longitudinal magneto-optical Kerr effect (MOKE) geometry, and the emission dynamics by time-domain THz spectroscopy (THz-TDS). In Gr/Co, the graphene interface induces perpendicular magnetic anisotropy; the phase of the THz waveforms is invariant with respect to the pumping side at a fixed field polarity, indicating demagnetization-driven emission. Under back-side pumping the amplitude increases by ≈1.5×, whereas front-side excitation reduces it by about a factor of two, consistent with differences in optical/THz absorption and interference. In Co/FeMn, the antiferromagnetic layer imposes pronounced in-plane uniaxial anisotropy and increases coercivity; a phase inversion upon switching the pumping side indicates a dominant inverse spin Hall effect. No exchange bias is observed at the selected thicknesses and without post-annealing. Additionally, an asymmetry of the THz hysteresis loops in Co/FeMn reveals even-in-magnetization contributions to the emission. These results underscore the central role of interface engineering in Co/AFM and Gr/Co stacks for controlling spin-to-charge conversion and optimizing THz-emitter performance.