Laser beam welding is used in many areas of industry and research. There are many strategies and approaches to further improve the weld seam properties in laser beam welding. Metallography is often needed to evaluate welded seams. Typically, the images are examined and evaluated by experts. The evaluation process qualitatively provides the properties of the welds. Particularly in times when artificial intelligence is being used more and more in processes, the quantization of properties that could previously only be determined qualitatively is gaining importance. In this contribution, we propose to use deep learning to perform semantic segmentation of micrographs of complex weld areas to achieve the automatic detection and quantization of weld seam properties. A semantic segmentation dataset is created containing 282 labeled images. The training process is performed with DeepLabv3+. The trained model achieves a value of around 95% for weld contour detection and 76.88% of mean intersection over union (mIoU).
26 September 2022 in Journal of Laser Applications
Nowadays, there is a strong and growing ambition to switch from combustion technology to battery-electric drives, and energy storage is spotlighted. Laser beam welding is an appropriate and favorable welding technology in battery production. Due to the high welding speed, the local heat input, the contact freeness efficient, and automatable processes can be established. Materials used in batteries for electrodes that have to be connected are commonly copper and aluminum. Specifically, copper is highly reflective for widely used infrared laser beam wavelengths. Furthermore, the thickness in the area of 10 μm is quite challenging to deal with, in terms of gap free clamping and avoidance of damage to the material as well as distortion during welding. There is a fine line regarding energy input between burning the material and generating a lack of fusion. In the presented research, welding approaches with different laser beam sources emitting laser beams with infrared wavelengths, various beam shapes, and welding modes (continuous and pulsed) are studied. A total of 40 copper foils with a thickness of 10 μm and 40 aluminum foils with a thickness of 15 μm are welded to similar sheet metals. Aim of the process development are welds with high quality and high connection widths to provide the best electric conductivity.
Laser beam brazing is an established manufacturing process due to its low heat input and esthetically appealing seams. However, brazing of materials with high oxygen affinity, such as aluminum alloys, requires the removal of surface oxides prior to the brazing process, commonly through the application of chemical fluxes that may be harmful to the environment and to health. The approach presented here dispenses with the use of fluxes and involves oxide layer removal by means of ns-pulsed laser radiation within an atmosphere that is adequate to an extreme high vacuum (XHV) in regard to the oxygen content. By doping the process gas with monosilane (SiH4), an oxygen content equivalent to an extreme high vacuum with an oxygen partial pressure below 10−20 mbar is realized. Hence, a subsequent reoxidation is actively prevented so that wetting of the base material by the filler material and consequent diffusion processes are enabled. The wetting angle between filler material and material is used to evaluate the effectiveness of laser-based deoxidation under an XHV-adequate atmosphere.
Welding by laser beam is a method for creating deep and narrow welds with low influence on the surrounding material. Nevertheless, the microstructure and mechanical properties change, and highly alloyed materials are prone to segregation. A new promising approach for minimizing segregation and its effects like hot cracks is introducing ultrasonic excitation into the specimen. The following investigations are about the effects of different ultrasonic amplitudes (2/4/6 µm) and different positions of the weld pool in the resonant vibration distribution (antinode, centered, and node position) for bead on plate welds on 2.4856 nickel alloy round bars (30 mm diameter) with a laser beam power of 6 kW. The weld is evaluated by visual inspection and metallographic cross sections. The experiments reveal specific mechanisms of interaction between melt and different positions regarding to the vibration shape, which influence weld shape, microstructure, segregation, cracks and pores. Welding with ultrasonic excitation in antinode position improves the welding results.
Fusion joining of stainless steel to copper without a filler material for pipe processing proves itself to be challenging due to the very different material properties of the joining partners and very heterogeneous characteristics in the weld metal due to different mixing ratios. One of the most common weld defects in this material combination is solidification cracking in the weld metal due to liquid copper accumulation between the stainless steel grain boundaries, which cannot withstand the tensile tensions while cooling down. Consequently, these cracks can reduce the mechanical properties, lead to leakages or cause faster corrosion. To prevent cracking, a precise control of the melting and mixing ratio of stainless steel and copper is needed. Laser beam welding offers many capabilities to influence the resulting weld metal shape and size as well as the mixing ratios with different approaches such as parameter optimization, inline process control, or the use of different beam shapes. This work shows different weld configurations and applications using sheets with thicknesses in the area of 1 mm and pipe samples. The main focus is on different solutions to influence the copper dilution and the weld metal geometry for solidification crack prevention. Therefore, a design of experiment approach and inline weld depth control using optical coherence tomography (OCT) data is used for the lap weld configuration to limit the copper dilution below 10 wt. % in steel dominated weld metals. Moreover, the benefits of adjustable intensity profiles for the butt weld configuration to control the shape and dimensions of the weld metal and mixing behavior with different power distributions in the laser beam welding spot are shown. The overall results indicate that solidification cracking in steel-copper joints can be influenced by different process approaches.
17 September 2021 in Journal of Laser Applications
The risk of weld defects increases when laser beam welding of round bars is performed in a rotational process. The reason is heat accumulation, which changes process conditions. The analysis of weld pool shape and weld defects in the course of a weld seam is essential for being able to evaluate the overall weld quality and to set up control measures. This study focuses on laser beam welding of round bars with partial welds and various welding speeds. The experiments are carried out with 1.7035 round bars of 30 mm diameter. For partial welds, a laser beam power of 6 kW and welding speed of 1 m/min are used for welding paths of 1/4, 1/2, and 3/4 of the circumference. Welding with various speeds is conducted with 0.5, 1.0, and 1.5 m/min and a constant energy per unit length of 240 kJ/m. The specimens are evaluated by metallographic microsections and scanning acoustic microscopy. The investigations reveal three major weld defects resulting from a gradient in linear welding speed between the specimen surface and the center and from heat accumulation due to specimen geometry. Porosity and hot cracks form under the surface and the weld root bulges, which also result in hot cracks. The weld depth increases to its final weld depth after approximately 1/8 of the circumference.