Flexible photovoltaic (PV) technology not only has high power efficiency but also is thin and lightweight, enabling seamless adaption to the surface of curved buildings. However, the distinctive spatial geometry of curved surfaces leads to inhomogeneous irradiance, causing electrical mismatch losses. This study examines the geometric origin of photoelectric mismatch through controlled indoor experiments on bare flexible CIGS cells in six configurations: flat, length convex, length concave, width convex, width concave, and length wavy. The tests were conducted under standard test conditions at central angles from 0° to 180° and in two laboratory orientations. A two-dimensional microfacet optical model, accounting for direct-beam projection, self-shading, and inter-arm mutual reflection, was developed and calibrated against the measurements, giving an R2 = 0.85 and RMSE = 5.1%. The results show that width-bending configurations retain a performance ratio (PR) above 60% over the tested angular range because the irradiance gradient is distributed across the current-collection path. In contrast, length bending aligns the gradient with the current path and leads to much larger mismatch losses. For the concave cases, mutual reflection improves performance at intermediate central angles, but this benefit is lost when self-shading becomes dominant beyond approximately 135°. The most severe case is length concave in the horizontal orientation at 180°, which retains only 43.4% of the flat-reference power, corresponding to a 56.6% loss and 319.7 mW of mismatch loss. These findings clarify how bending direction, curvature, and orientation affect cell-level mismatch and provide design guidance for curved CIGS BIPV systems.
Flexible photovoltaic modules offer an innovative approach for Building Integrated Photovoltaics (BIPV) on non-planar envelopes. However, the dynamic outdoor environment aggravates the photoelectric mismatch mechanism caused by complex curved geometries. This study experimentally investigates the outdoor experimental investigation into the dynamic electrical and thermal performance of large-scale curved CIGS modules equipped with bypass diodes. Six representative configurations—flat, length-convex(lgvx), length-concave(lgcv), width-convex(wdvx), width-concave(wdcv), and wavy—were continuously monitored under real weather conditions in Hefei, China. The results indicate that while flat modules maintain the highest daily energy yield (453.32 Wh) , the wdvx in longitudinal direction exhibits exceptional adaptability, achieving an average Performance Ratio (PR) of 91.46% and outperforming the flat type during low solar altitude periods in the day. Infrared thermal imaging reveals significant temperature gradients driven by the mismatch effect, with the lgcv module reaching a peak temperature of 65.88°C. Furthermore, the I-V characteristic curves demonstrate that non-uniform self-shading triggers bypass diode activation, resulting in severe step-like current drops and multiple power peaks in concave and wavy shapes. These findings offer crucial practical guidelines for optimizing cell layout and thermal management in curved BIPV envelops.
Flexible photovoltaic(PV) technology not only has high power efficiency but also is thin and lightweight, enabling seamless adaption to the surface of curved buildings. However, the distinctive spatial geometry of curved surfaces leads to inhomogeneous irradiance, causing electrical mismatch losses. This paper presents a systematic indoor experimental study on the electrical performance of Copper Indium Gallium Selenide (CIGS) cells under various bending configurations, including length-convex (lgvx), length-concave (lgcv), width-convex (wdvx), and width-concave (wdcv). Tests were conducted under standard testing conditions (1000 W/m², 25°C) with central angles ranging from 0° to 180° and placed in longitudinal and horizontal orientations, respectively. Results indicate that width-bending configurations generally outperform length-bending ones due to lower mismatch losses. For width-bending, concave forms exhibit higher power output than convex forms due to a mutual reflection mechanism. Conversely, length-concave forms manifest the highest power mismatch loss (up to 319.70 mW at 180°) due to significant self-shading. These findings provide critical design guidelines for optimizing cell layouts in curved BIPV systems.