Suhut Alexander Situmorang

Mr. Suhut Alexander Situmorang

orcid

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
22 January 2022 in Polymers
Verified
Journal Article
Open access
PDF file
SGSaharman Gea
Saharman Gea
BABoy Attaurrazaq
Boy Attaurrazaq
SSSuhut Alexander Situmorang
Suhut Alexander Situmorang
APAverroes Fazlur Rahman Piliang
Averroes Fazlur Rahman Piliang
SHSunit Hendrana
Sunit Hendrana
SGstergios goutianos
stergios goutianos
High temperature is required in carbon fiber synthesis in the carbonization step. However, direct high-temperature heating without the presence of additive materials would affect the yield and structure of carbon fibers produced. Thus, this study aims to synthesize carbon fibers from poly-vinyl alcohol (PVA), as the precursor and reducing agent, using silver nanoparticles (SNP) from silver nitrate (AgNO3) as additives. The pre-treatment of PVA was performed in three steps, i.e., mixing PVA/AgNO3, electrospinning, and iodination. The interaction of PVA and AgNO3 was assessed by FTIR, and SEM was used to characterize the electro-spun fibers prior and after iodination; Raman spectrophotometer was carried out to confirm the yield of carbon fibers. There was reduction in oxygen groups (3000–3800 cm−1) and emergence of –C=O (1100 cm−1) and –C=C– (1627 cm−1) functional groups, indicating formation of carbon layers. Based on the DT/GA results, the silver nanoparticles reduce the need of high temperature with optimum carbonization at 350 °C and lead to the formation of more regular graphene layers. Graphene layers with a size distribution of 0.438 nm and well-organized structures were successfully formed, and the Raman shifting showed higher intensities of G and G’ bands in the presence of Ag. Based on DT/GA results, the yield of carbon fibers with iodinated PVA fibers and SNP as additive had higher rates around 800 µg/min, reaching 33% at 500 °C. Thus, it is demonstrated that iodinated PVA/AgNO3 samples can significantly improve carbon fiber yield at low temperatures.