Nanocomposite film of poly(vinyl alcohol) (PVA) incorporated with bacterial cellulose nanocrystals (BCNCs) and magnetite nanoparticles (Fe3O4) is reported in this study. The BCNC-Fe3O4 nanoparticles and PVA film was prepared by in situ synthesis technique using chemical co-precipitation. Different concentrations of BCNC-Fe3O4 (20%, 40% and 60% w/w) were mechanically dispersed in PVA solution to form the nanocomposite film. Transmission electron microscopy (TEM) analysis of BCNC-Fe3O4 nanoparticles showed irregular particle sizes ranging from 4.93 to 30.44 nm with an average size distribution of 22.94 nm. The presence of characteristic functional groups of PVA, BCNC and Fe3O4 were confirmed by Fourier transform infrared (FTIR) spectroscopy and X-ray diffraction (XRD) analysis. Scanning electron microscope (SEM) attached energy dispersive spectroscopy (EDS) and vibrating sample magnetometer (VSM) analysis revealed that, the iron content and magnetic property increased with increasing BCNC-Fe3O4 content. The saturation magnetizations (MS) value increased from 5.14 to 11.56 emu/g. The PVA/ BCNC-Fe3O4 at 60% showed the highest Young’s modulus value of 2.35 ± 0.16 GPa. The prepared film could be a promising polymeric nanomaterial for various magnetic-based applications and for the design of smart electronic devices.
21 December 2024 in International Journal of Biological Macromolecules
The objective of this study was to investigate the morphological and chemical properties of hemp bast RPF1 variety fiber to be used as a potential raw material for filter paper production.
The aim of this study was to create a reinforced composite wood-based panel that would be leaned towards the environment Plywood was used as a core material and fiber-reinforced polymer was used as a reinforcement. Conventional resin for the fiber-reinforced polymer was substituted with polyvinyl acetate (PVAC), which has several advantages, such as a lower price, easier handling, and better degradability. The second chosen component, basalt fiber, is cost attractive and environmentally friendly. The combination of one and two layers of fabric with three fiber fractions and 4 mm thick plywood was investigated. The best results were achieved with two layers of fabric and the highest fiber fraction. The improvements of the ultimate bending load and bending stiffness of the plywood in the perpendicular direction were 305% and 325%, respectively. The ultimate load and stiffness of the parallel direction were improved by 31% and 35%, respectively. However, specimens always failed in the compressional zone. The highest reinforcing effect was found with the impact test: The energy required to fracture specimens increased by 4213% and 6150% for one and two layers of fabric, respectively. In conclusion, specimens exhibited high ductility due to the PVAC and basalt fiber. The amount of work and energy required to cause fractures was extensive.