The use of composite resins in dentistry is well accepted for restoring anterior and posterior teeth. Many polishing protocols have been evaluated for their effect on the surface roughness of restorative materials. This study compared the effect of different polishing systems on the surface roughness of microhybrid composites. Thirty-six specimens were prepared for each composite [Charisma® (Heraeus Kulzer), Fill Magic® (Vigodent), TPH Spectrum® (Dentsply), Z100® (3M/ESPE) and Z250® (3M/ESPE)] and submitted to surface treatment with Enhance® and PoGo® (Dentsply) points, sequential Sof-Lex XT® aluminum oxide disks (3M/ESPE), and felt disks (TDV) combined with Excel® diamond polishing paste (TDV). Average surface roughness (Ra) was measured with a mechanical roughness tester. The data were analyzed by two-way ANOVA with repetition of the factorial design and the Tukey-Kramer test (p<0.01). The F-test result for treatments and resins was high (p<0.0001 for both), indicating that the effect of the treatment applied to the specimen surface and the effect of the type of resin on surface roughness was highly significant. Regarding the interaction between polishing system and type of resin used, a p value of 0.0002 was obtained, indicating a statistically significant difference. A Ra of 1.3663 was obtained for the Sof-Lex/TPH Spectrum interaction. In contrast, the Ra for the felt disk+paste/Z250 interactions was 0.1846. In conclusion, Sof-Lex polishing system produced a higher surface roughness on TPH Spectrum resin when compared to the other interactions.
Clinical Relevance: Lower depth of cure with the LED unit, compared to the QTH unit, is associated with different light scattering due to differences in spectral emission.
The aim of this study was to verify the influence of an experimental heat treatment (170ºC/10 min) using a casting furnace on the mechanical properties (hardness and flexural strength) of 2 commercial direct resin composites (TPH Spectrum and Filtek P60) compared to a commercial indirect resin system (BelleGlass). Heat treatment temperature was determined after thermal characterization by thermogravimetry (TG) and differential scanning calorimetry (DSC). Data was analyzed by ANOVA and Tukey's test at 5% significance level. There was statistical significance for the main factor heat treatment (p=0.03) and composite (p=0.02), for flexural strength. For Knoop hardness, only the main factor composite was statistically significant (p=0.00). P60 presented higher hardness than TPH. No statistically significant correlation between mechanical properties tested was detected. Based on these results, it was possible to conclude that heat treatment influenced flexural strength of direct composites, while it was not observed for hardness. The association of direct composites with a simple post-cure heat treatment may be an alternative for current indirect composite systems, although more studies are needed to verify other properties of the composites for this application.
This study evaluated the Vickers hardness (VHN) and diametral tensile strength (DTS) of the composite Z100 (3M ESPE) cured with: Quartz-Tungsten-Halogen light curing unit (QTH) (700mW/cm2- 40 s) and Argon laser (1,000mW/cm2- 10 s). Specimens of 2 mm depth and 8 mm diameter were immersed for 30 days at 37°C in different storage means: water, alcohol, acetic acid, propionic acid and dry (control). The DTS (n = 8) was determined with a crosshead speed of 0.5 mm/min. The VHN (n = 8) test was carried out using a 50 g load for 60 s. Statistical analysis was performed by two-way ANOVA and Tukey's test (α = 0.05). The relationship between VHN and DTS was observed by Pearson correlation. The light source was not significant in both tests (VHN: P < 0.18; DTS: P < 0.92), but the factor storage showed significance (P < .001). Mechanical properties of the control group were statistically superior to those of the other storage groups (VHN = 102.2; DTS = 42.3 MPa). The alcohol group showed the lowest VHN (93.3) and DTS (33.8 MPa) values, which were similar to values for propionic (VHN = 97.5; DTS = 35.9 MPa) and acetic acids (VHN = 97.8; DTS = 36.1 MPa), but different from that of water (VHN = 102.2; DTS = 42.3 MPa). The relationship between VHN and DTS values presented a positive correlation (r2 = 0.90; P < 0.01). (J. Oral Sci. 49, 61-66, 2007)
3 December 2009 in Journal of Esthetic and Restorative Dentistry