In this work, nanocomposite samples of polyaniline (PANI) and lead sulfide nanoparticles (PbSNPs) were prepared, utilizing the solution preparation method, for implantation in energy storage elements. The PANI/PbS films were irradiated by different fluences of oxygen beam: 5 × 1016, 10 × 1016, and 15 × 1016 ions.cm−2. The composite was investigated by XRD, SEM, DSC, and FTIR. After ion irradiation, the Tg and Tm values decreased by 4.8 °C and 10.1 °C, respectively. The conductivities, electrical impedances, and electrical moduli of untreated and irradiated samples were examined in frequencies ranging from 102 Hz to 5 MHz. Moreover, the ion beam caused a modification in the dielectric characteristics of PANI/PbS. The dielectric constant ε′ was improved from 31 to 611, and the electrical conductivity increased from 1.45 × 10−3 S/cm to 25.9 × 10−3 S/cm by enhancing the fluence to 15 × 1016 ions.cm−2. Additionally, the potential energy barrier, Wm, decreased from 0.43 eV to 0.23 eV. The induced changes in the dielectric properties and structural characteristics of the PANI/PbS samples were determined. These modifications provide an opportunity to use irradiated PANI/PbS samples for several applications, including microelectronics, batteries, and storage of electrical energy.
2 September 2023 in Optical and Quantum Electronics
The grain size impact on the behavior of ZnO–Bi2O3–Mn2O3 varistors was determined in this study. Samples with different sintering temperatures and times were prepared via traditional ceramic methodology, and their properties were described. Results exhibited that various temperatures and times of the sintering process had considerable effects on the varistors. In particular, the growth of ZnO grains was improved at a minimal-temperature sintering process of 900 °C for 1 h. Significant solid-state reaction even at lower sintering temperatures perhaps caused the surface characteristics of ZnO nanoparticles. Vickers indentation analyses were applied to define the fracture toughness and hardness of the samples. Hardness diminished with the growth of ZnO grain. Fracture toughness did not exhibit any change with the increase in grain size (~ 5.1 MPam0.5) up to 1.6 μm for WZ-V and 3.5 μm 20Z-V. Above these grain sizes, a spontaneous conversion from hexagonal to monoclinic phase occurred. WZ-V and 20Z-V samples were used to investigate the analogous bending strength at 1152 and 1148 MPa, respectively. The structural coarsening desired for realizing significant grain size led to increased scattering strength values, as evidenced by lesser Weibull modulus (9.23 vs. 5.10). Variations in the mechanical behavior of the investigated varistors with different grain sizes were demonstrated, and their probable reasons were discussed in brief.