To overcome the drawbacks of solvent evaporation and leakage from the liquid electrolyte in dye-sensitized solar cells (DSSCs), a polymer gel electrolyte (PGE), based on polydopamine (PDA)-modified electrospun polyvinylidene fluoride (PVDF) nanofibers, [email protected], was prepared and applied in quasi-solid DSSCs (QS-DSSCs). The PDA coating increased the wettability of the liquid electrolyte by improving the distribution of the ionic liquid electrolyte. This, in turn, enhanced the ion conductivity of the PGE as well as the stability of QS-DSSC. The [email protected] nanofiber membrane exhibited a satisfactory ultimate tensile strength of 9.3 MPa with a failure elongation of 130%. Such high toughness provided excellent mechanical support for the PGE. Owing to the unique pore connected structure of nonwoven nanofibers as well as the reduced surface tension with the liquid electrolytes, the PGE-based QS-DSSC retained 95.7% of the short circuit current from the liquid-electrolyte-based DSSC and showed an energy conversion efficiency of 8.26%. No significant impacts were observed for the open-circuit voltage and fill factor. More importantly, the QS-DSSCs using [email protected] PGE showed a significantly improved solar cell stability under both indoor and outdoor conditions.
To obtain new highly efficient and stable quasi-solid dye-sensitized solar cells (QS-DSSCs) that can meet the requirements for the large-scale commercial application of solar cells, we have developed a novel quasi-solid-state electrolyte, based on an electrospun polyvinylidene fluoride (PVDF) membrane. The structure and properties of electrospun PVDF membranes were characterized by scanning electron microscopy (SEM), Brunauer–Emmett–Teller (BET), thermogravimetric (TG), and mechanical testing. The results indicate that the electrospun PVDF membrane has a three-dimensional network structure with extremely high porosity, which not only acts as a barrier to prevent electrolyte leakage but also provides a channel for the transmission of ions in the electrolyte, thereby effectively guaranteeing the high photoelectric conversion efficiency of the cells. The membrane was observed to withstand the conditions of hot-press (110 °C), and exhibited good thermal stability and mechanical strength, which are critical for the long-term stability and safety of the cells. The photovoltaic characteristics and stabilities of QS-DSSCs were compared with DSSCs based on an ionic liquid electrolyte (L-DSSC). QS-DSSCs with an 80 μm thick nanofiber electrolyte membrane showed a conversion efficiency of 8.63%, whereas an identical cell based on the corresponding ionic liquid electrolyte showed an efficiency of 9.30%. The stability test showed that, under indoor and outdoor conditions, after 390 h, the L-DSSCs failed. Meanwhile, the QS-DSSCs also maintained 84% and 77% of the original efficiency. The results show that, compared to the liquid electrolyte, the design of the quasi-solid electrolytes based on electrospun PVDF nanofiber membrane not only demonstrates the high conversion efficiency of DSSCs but also enhances the stability of the DSSCs, which provides the possibility for the fabrication of solar cells with higher efficiency and stability.
1 October 2020 in International Journal of Hydrogen Energy
Carboxylic contained zeolitic imidazolate frameworks (ZIF-COOH) were designed and synthesized using 1H-Imidazole-2-carboxylic acid and Zn(NO3)2·6H2O. The ZIF-COOH was then applied in the fabrication of composite membranes with sulfonated polyether ether ketone (SPEEK) (SPEEK/ZIF-COOH). The properties of the composite membranes, including mechanical strength, proton conductivity, and methanol permeability were studied. The incorporation of ZIF-COOH generated a significant effect on SPEEK/ZIF-COOH composite membranes, due to the special structure and compositional characteristics of ZIF-COOH. In particular, the tensile strength of SPEEK/ZIF-COOH-5 showed an enhancement of 44.1 MPa, which was 42% higher than the pristine SPEEK. Simultaneously, the proton conductivity displayed an improvement of 46% as compared to the SPEEK. Most importantly, the methanol permeability values decreased to 1.1 × 10−7 cm2 s−1, which was only a tenth of the value of SPEEK.