The paper reports the fabrication and characterization of ZnO-based interdigitated metal–semiconductor–metal (MSM) and metal–insulator–semiconductor–insulator–metal (MISIM) ultraviolet photodetectors. The ZnO thin film was grown on a p-type Si ⟨1 0 0⟩ substrate by the sol–gel technique. With applied voltage in the range from −3 to 3 V we estimated the contrast ratio, responsivity, detectivity and quantum efficiency of the photodetectors for an incident optical power of 0.1 mW at 365 nm ultraviolet wavelength. The I–V characteristics were studied and the parameters such as ideality factor, leakage current and barrier height were extracted from the measured data. For Au/Cr/SiO2/ZnO/SiO2/Al (MISIM) structure the product (mχ) of the tunnelling effective electron mass (m) and the mean tunnelling barrier height (χ) was also extracted.
The article reports fabrication, characterization, and testing of the performance of ZnO-based metal-insulator-semiconductor (MIS) Schottky barrier ultraviolet photodetectors under varying thermal treatment. The ZnO thin film was grown on p-type Si substrate by using sol-gel technique. The electrical and optical characteristics of MIS photodetector were studied. The study revealed that the performance of the device improves with increasing postmetal deposition annealing temperature up to approximately. For annealing temperature beyond the performance of the device degrades drastically. The variation in the electrical and photoresponse properties of MIS photodetector can be attributed to combined effects of interfacial reaction and phase transition during the annealing process.
The authors report on characterization of Pd/ZnO thin film Schottky contacts based UV photodetector fabricated by two methods. The ZnO film was grown on p-type Si ⟨100⟩ substrate by using vacuum thermal evaporation and sol-gel methods. With applied voltage in the range from −2 to +2 V we estimated the photocurrent, contrast ratio, responsivity, and quantum efficiency of the photodetectors for an incident optical power of 0.1 mW at 365 nm ultraviolet wavelength. The current–voltage characteristics were studied and the parameters such as ideality factor, leakage current, and barrier height of the Schottky contacts were extracted from the measured data. The surface morphology and the structural properties of the thin film were studied by atomic force microscope and scanning electron microscope. The bandgap of ZnO is evaluated from the absorbance spectra of ZnO thin film obtained by using double beam spectrophotometer. For the investigation of the surface chemical bonding, x-ray photoelectron spectroscopy measurements were also performed. The study revealed that sol-gel derived devices exhibit better photoresponse as compared to those using thin film deposited by vacuum deposition technique.
21 October 2016 in Journal of Electronic Materials
Three methods were used to fabricate ZnO-based room temperature liquid petroleum gas (LPG) sensors having interdigitated metal-semiconductor-metal (MSM) structures. Specifically, devices with Pd Schottky contacts were fabricated with: (1) un-doped ZnO active layers; (2) Pd-doped ZnO active layers; and (3) un-doped ZnO layers on top of Pd microstructure arrays. All ZnO films were grown on p-type Si(111) substrates by the sol-gel method. For devices incorporating a microstructure array, Pd islands were first grown on the substrate by thermal evaporation using a 100 μm mesh shadow mask. We have estimated the sensitivity of the sensors for applied voltage from