Understanding nanoparticle growth mechanisms is crucial for the synthesis of nanocrystals with desired biological and chemical properties. Growth of nanocrystals by oriented attachment (OA) is frequently reported as a method supplementary to the classical growth by Ostwald ripening (OR) process. In this work, ZnO nanoparticles (NPs) were prepared by wet chemical method. Size/shape evolution of ZnO NPs in ethanol solution was systematically studied using transmission electron microscopy (TEM), dynamic light scattering (DLS), and X-ray diffraction (XRD). In addition, a detailed process of the nanoparticle growth-based OA mechanism is discussed. Results revealed that reaction conditions affect size/shape of NPs and change their surface structure: prior to OA, the surface of adjacent particles transformed into their “rough” states. We proved that stability of the solution was significantly improved in this state. Such a state is important to design nanoparticles with high stability and as nano-suspensions with special physical and/or chemical properties. This state is a critical step in enhancing OA process.
ZnO nanoparticles are widely used in biological, chemical, and medical fields, but their toxicity impedes their wide application. In this study, pristine ZnO NPs (~ 7 nm; ~ 18 nm; ~ 49 nm) and lipid-coated ZnO NPs (~ 13 nm; ~ 22 nm; ~ 52 nm) with different morphologies were prepared by chemical method and characterized by TEM, XRD, HRTEM, FTIR, and DLS. Our results showed that the lipid-coated ZnO NPs (~ 13 nm; ~ 22 nm; ~ 52 nm) groups improved the colloidal stability, prevented the aggregation and dissolution of nanocrystal particles in the solution, inhibited the dissolution of ZnO NPs into Zn2+cations, and reduced cytotoxicity more efficiently than the pristine ZnO NPs (~ 7 nm; ~ 18 nm; ~ 49 nm). Compared to the lipid-coated ZnO NPs, pristine ZnO NPs (~ 7 nm; ~ 18 nm; ~ 49 nm) could dose-dependently destroy the cells at low concentrations. At the same concentration, ZnO NPs (~ 7 nm) exhibited the highest cytotoxicity. These results could provide a basis for the toxicological study of the nanoparticles and direct future investigations for preventing strong aggregation, reducing the toxic effects of lipid-bilayer and promoting the uptake of nanoparticles by HeLa cells efficiently.
The increasing metal release into the environment warrants investigating their impact on plants, which are cornerstones of ecosystems. Here, Lactuca sativa L. (lettuce) seedlings were exposed hydroponically to different concentrations of silver ions and nanoparticles (Ag NPs) for 25 days to evaluate their impact on plant growth. Seedlings taking Ag+ ions showed an increment of 18% in total phenolic content and 12% in total flavonoid content, whereas under Ag NPs, 7% free radical scavenging activity, 12% total phenolic contents (TPC), and 10% total reducing power are increased. An increase in 31% shoot length, 25% chlorophyll, 11% carbohydrate, and 16% protein content of the lettuce plant is observed in response to Ag NPs, while silver nitrate (AgNO3) has a reduced 40% growth. The lettuce plant was most susceptible to toxic effects of Ag+ ions at a lower concentration, i.e., 0.01 mg/L, while Ag NPs showed less toxicity, only when higher concentrations >100 mg/L were applied. Further, biomolecules other than antioxidant enzymes showed higher phytotoxicity for Ag+ ions, followed by Ag NPs with the concentration of 25, 50, and 100 mg/L compared to the control. Thus, moderate concentrations of Ag NPs have a stimulatory effect on seedling growth, while higher concentrations induced inhibitory effects due to the release of Ag+ ions. These results suggest that optimum metallic contents are desirable for the healthier growth of plants in a controlled way.
Withania coagulans contains a complex mixture of various bioactive compounds. In order to reduce the complexity of the plant extract to purify its phytochemical biomolecules, a novel fractionation strategy using different solvent combination ratios was applied to isolate twelve bioactive fractions. These fractions were tested for activity in the biogenic synthesis of cobalt oxide nanoparticles, biofilm and antifungal activities. The results revealed that plant extract with bioactive fractions in 30% ratio for all solvent combinations showed more potent bioreducing power, according to the observed color changes and the appearance of representative absorption peaks at 500–510 nm in the UV-visible spectra which confirm the synthesis of cobalt oxide nanoparticles (Co3O4 NPs). XRD diffraction was used to define the crystal structure, size and phase composition of the products. The fractions obtained using 90% methanol/hexane and 30% methanol/hexane showed more effectiveness against biofilm formation by Pseudomonas aeruginosa and Staphylococcus aureus so these fractions could potentially be used to treat bacterial infections. The 90% hexane/H2O fraction showed excellent antifungal activity against Aspergillus niger and Candida albicans, while the 70% methanol/hexane fraction showed good antifungal activity for C. albicans, so these fractions are potentially useful for the treatment of various fungal infections. On the whole it was concluded that fractionation based on effective combinations of methanol/hexane was useful to investigate and study bioactive compounds, and the active compounds from these fractions may be further purified and tested in various clinical trials.