Xiaoma Ding

Mr. Xiaoma Ding


Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 September 2019 in RSC Advances
Verified
Journal Article
Open access
PDF file
MQMengmeng Qiao
Mengmeng Qiao
HKHaijuan Kong
Haijuan Kong
XDXiaoma Ding
Xiaoma Ding
LZLuwei Zhang
Luwei Zhang
XDXiaoma Ding
Xiaoma Ding
In this paper, graphene oxide (GO) was successfully prepared by the modified Hummers’ method and then uniformly dispersed in an aqueous solution containing a small amount of polyvinyl alcohol (PVA) as an adhesive. The solution was uniformly coated on the surface of polyacrylonitrile (PAN) fibers and then the fibers were pre-oxidized at 240 °C for 20 min in the air. The pre-oxidation degree of PAN fibers and fibers coated with different contents of GO was analyzed by the Fourier transform infrared (FT-IR) spectroscopy, differential scanning calorimetry (DSC), X-ray diffraction (XRD) and thermogravimetric analysis (TGA). In addition, the surface and cross-section of PAN fibers before and after pre-oxidation were observed by scanning electron microscopy (SEM). The experimental results showed that the presence of GO coatings significantly improved the pre-oxidation degree of PAN fibers, at the same time, the pre-oxidation degree of PAN fibers increased with the increase of GO contents from 0.2 to 1.0 mg ml−1. The cross-section morphology of the pre-oxidized PAN fibers revealed that the degree of pre-oxidation inside fibers was uniform. This was because the GO coatings acted as a medium to transfer heat, removing the heat released during the pre-oxidation process and increasing the pre-oxidation degree.

1 October 2019 in RSC Advances
Verified
Journal Article
Open access
PDF file
XDXiaoma Ding
Xiaoma Ding
HKHaijuan Kong
Haijuan Kong
MQMengmeng Qiao
Mengmeng Qiao
LZLuwei Zhang
Luwei Zhang
XDXiaoma Ding
Xiaoma Ding
In this article, the surface modification of AF with epichlorohydrin assisted by supercritical CO 2 was investigated in order to improve the interface combination property between an aramid fiber and an epoxy resin matrix.

10 May 2019 in Polymers
Verified
Journal Article
Open access
PDF file
XDXiaoma Ding
Xiaoma Ding
HKHaijuan Kong
Haijuan Kong
MQMengmeng Qiao
Mengmeng Qiao
ZHZhifeng Hu
Zhifeng Hu
XDXiaoma Ding
Xiaoma Ding
In order to obtain F-III fibers with high mechanical properties, pristine F-III fibers were hot drawn at the temperature of 250 °C, pressure of 14 MPa, tension of 6 g·d−1, and different times, which were 15 min, 30 min, 45 min, 60 min, 75 min, 90 min, and 105 min, respectively, in supercritical carbon dioxide (Sc-CO2) in this article. All the samples, including the pristine and treated F-III fibers, were characterized by a mechanical performance tester, wide-angle X-ray scattering (WAXS), small-angle X-ray scattering (SAXS), and thermogravimetric analysis (TGA). The results showed that the thermal stability of F-III fibers was enhanced to some extent, and the tensile strength and modulus of F-III fibers had great changes as the extension of treatment time during hot drawing in Sc-CO2, although the treatment temperature was lower than the glass transition temperature (Tg) of F-III fibers. Accordingly, the phase fraction, orientation factor fc of the (110) crystal plane, fibril length lf, and misorientation angle Bφ of all the samples were also investigated. Fortunately, the hot drawing in Sc-CO2 was successfully applied to the preparation of F-III fibers with high mechanical properties.

9 September 2021 in Journal of Adhesion Science and Technology
Verified
Journal Article
Closed access
ZHZhifeng Hu
Zhifeng Hu
HKHaijuan Kong
Haijuan Kong
XDXiaoma Ding
Xiaoma Ding
This study developed a kind of non-woven carbon tissue reinforced adhesive film (NWCTRAF) with high bonding strength and reliability by interleaving the NWCT into the adhesive film. The manufacturing process, bonding strength, Weibull distribution, metallography of cross-section, and fracture surface morphology of NWCTRAF specimens were investigated. The results showed that the average bonding strength and Weibull characteristic strength (WCS) of single lap joint (SLJ) were 27.4a and 28.2 MPa, which increased by 17.6% and 15.1%, respectively compared with the blank specimen, and the Weibull modulus risen from 9.51 to 18.72, which indicated that NWCTRAF specimens had higher bonding reliability. The mechanism of micro-crack formation was obtained by analyzing the cross-section of loading 95% WCS without visible damage. The metallographic section showed that the microcracks of the blank specimen originated from the interface between carbon fiber-reinforced polymer (CFRP) and adhesive layer, while the microcracks of the NWCTRAF specimen originated from the resin-rich regions between the carbon fiber fabric layers in CFRP. Typical failure modes were gained from optical microscope and SEM. Failure modes of blank specimen included more interface failure of CFRP-adhesive and Al-adhesive, while NWCTRAF specimen had more carbon fiber tearing and delamination of CFRP. The fracture morphology of adhesively cohesive failure included the pull-out of short carbon fibers and the appearance of rough and multi-stage resin in the NWCTRAF specimen, which improved the toughness of the adhesive layer. The bridging effect of short carbon fibers in the NWCTRAF disperse and transfer stress to CFRP and fail at resin-rich regions of CFRP, decrease the bonding interface's direct failure, and improve the bonding strength and reliability.

26 February 2019 in Materials
Verified
Journal Article
Open access
PDF file
XDXiaoma Ding
Xiaoma Ding
HKHaijuan Kong
Haijuan Kong
MQMengmeng Qiao
Mengmeng Qiao
ZHZhifeng Hu
Zhifeng Hu
XDXiaoma Ding
Xiaoma Ding
F-III fibers were treated at different pressures in supercritical carbon dioxide fluid and all samples including untreated and treated F-III fibers were characterized by a mechanical performance tester, wide-angle X-ray scattering and small-angle X-ray scattering. By studying the relationship between mechanical performance and microstructural changes of the samples, it was found that microstructural change was the main cause of variation in mechanical performance. Results revealed that the maximum tensile strength and modulus of F-III fibers were acquired at 14 MPa within the pressure range of 8 MPa to 16 MPa when the temperature, tension and time were 250 °C, 6 g·d−1 and 40 min, respectively. Correspondingly, the microstructures of the samples, including the phase fraction, crystal size, orientation factor, fibril radius, fibril length and misorientation angle, have been investigated. It was fortunate that the supercritical carbon dioxide fluid could be used as a medium during the hot-stretch process to improve the mechanical performance of F-III fibers, although the treatment temperature was lower than the glass transition temperature of the F-III fibers.