The mechanical properties of Ti alloys are changed significantly with the addition of interstitial elements, such as oxygen. Because oxygen is a strong stabilizer of the α phase and has an effect on hardening in a solid solution, it has aroused great interest in the biomedical area. In this paper, Ti-Zr alloys were subjected to a doping process with small amounts of oxygen. The influence of interstitial oxygen in the structure, microstructure and some selected mechanical properties of interest for use as biomaterial and biocompatibility of the alloys were analyzed. The results showed that in the range of 0.02 wt% to 0.04 wt%, oxygen has no influence on the structure, microstructure or biocompatibility of the studied alloys, but causes hardening of the alloys, increasing the values of the microhardness and causing variation in the elasticity modulus values.
The Ti–15Mo alloy has its mechanical properties strongly altered by heat treatments and by addition of interstitial elements, such as, oxygen, for example. In this sense, the objective of this paper is to analyze the effect of the introduction of oxygen in selected mechanical properties and the biocompatibility of Ti–15Mo alloy. The samples used in this study were prepared by arc-melting and characterized by density measurements, X-ray diffraction, scanning electron microscopy, microhardness, modulus of elasticity, and biocompatibility tests. Hardness measurements were shown to be sensitive to concentration of oxygen. The modulus results showed interstitial influence in value; this was verified under several conditions to which the samples were exposed. Cytotoxicity tests conducted in vitro showed that the various processing conditions did not alter the biocompatibility of the material.
This study aimed to produce Ti-15Nb alloy with a low elastic modulus, verify its biocompatibility, and determine whether the alloy indirectly influences cellular viability and morphology, as well as the development of the osteogenic phenotype in cells cultured for 2, 3, and 7 days derived from rat calvarias. Two heat treatments were performed to modify the mechanical properties of the alloy where the Ti-15Nb alloy was heated to 1000 °C followed by slow (−5 °C/min) (SC) and rapid cooling (RC). The results of structural and microstructural characterization (XRD and optical images) showed that the Ti-15Nb alloy was of the α + β type, with slow cooling promoting the formation of the α phase and rapid cooling the formation of the β phase, altering the values for the hardness and elastic modulus. Generally, a more significant amount of the α phase in the Ti-15Nb alloy increased the elastic modulus value but decreased the microhardness value. After the RC treatment, the results demonstrated that the Ti-15Nb alloy did not present cytotoxic effects on the osteogenic cells. In addition, we did not find variations in the cell quantity in the microscopy results that could suggest cell adhesion or proliferation modification.
25 August 2016 in Microscopy Research and Technique