Stress relief treatment before machining and sawing aluminium direct chill cast products is required to avoid uncontrolled distortion, crack formation and significant safety concerns due to the presence of thermally induced residual stresses created during casting. Numerical models have been developed to compute these residual stresses and yet have only been validated against measured surface distortions. In the present contribution, the variations in residual strains and stresses have been measured using neutron diffraction and hole drilling strain gage in two AA 6063 grain refined cylindrical billet sections cast at two casting speeds. The measured residual stresses compare favourably with the numerical model, in particular the depth at which the axial and hoop stresses change sign. Such results provide insight into the development of residual stresses within castings and show that the stored elastic energy varies linearly with the casting speed, at least within the range of speeds that correspond to production conditions.
The rigidity temperature of a solidifying alloy is the temperature at which the solid plus liquid phases are sufficiently coalesced to transmit long range tensile strains and stresses. It determines the point at which thermally induced deformations start to generate internal stresses in a casting. As such, it is a key parameter in numerical modelling of solidification processes and in studying casting defects such as solidification cracking. This temperature has been determined in Al-Cu alloys using in situ neutron diffraction during casting in a dog bone shaped mould. In such a setup, the thermal contraction of the solidifying material is constrained and stresses develop at a hot spot that is irradiated by neutrons. Diffraction peaks are recorded every 11 s using a large detector, and their evolution allows for the determination of the rigidity temperatures. We measured rigidity temperatures equal to 557 °C and 548 °C, depending on cooling rate, for a grain refined Al-13 wt% Cu alloy. At high cooling rate, rigidity is reached during the formation of the eutectic phase and the solid phase is not sufficiently coalesced, i.e., strong enough, to avoid hot tear formation.
9 July 2015 in Metallurgical and Materials Transactions A