Carbon nanotubes (CNTs) reinforced aluminum matrix nanocomposites were fabricated by Accumulative Roll Bonding (ARB). The surface morphologies, mechanical properties, grains texture and orientation of the Al/CNTs nanocomposites were characterized, and the mechanisms and influences of CNTs contents and ARB cycles on the mechanical performance and grain textures of Al/CNTs were investigated and revealed. The strength of the composites rose with increase of the CNTs content, and the ARB cycles showed a 26% improvement when the CNTs content varied from 0 to 1 volume percent (vol.%). The increase in the mass fraction of the carbon nanotubes made the grain distribution in the Al/CNTs nanocomposite samples more diffuse. Besides, the stable texture of the hot rolled crystal grains on the α orientation are constantly turning to {011}< 011> with the mass fraction of the reinforcing phase increased.
1 June 2017 in Journal of Nanoscience and Nanotechnology
In present work, magnesium matrix nanocomposites (MMNC) containing 2 wt.%CNTs were fabricated through accumulative roll bonding (ARB). The microstructure and mechanical properties of Mg/2 wt.%CNTs nanocomposites are reported for various ARB cycles. To evaluate microstructure of the nanocomposites, the field emission scanning electron microscope (FESEM), X-ray diffractometer and transmission electron microscope (TEM) were applied. After fourteen ARB cycles, the nanocomposite showed a homogeneous distribution of reinforcements and significant reduction in average matrix grain size. Meanwhile, the nanocomposite revealed higher percentage of substructured grains and lower intensity of basal texture as compared to monolithic Mg. Mechanical properties were investigated through tensile and microhardness tests. The strength and elastic modulus and microhardness of Mg/2 wt.%CNTs were found to improve significantly from eight ARB cycles and reach maximum values at fourteen ARB cycles. The ultimate tensile strength, yield strength, microhardness and elastic modulus of Mg/2 wt.%CNTs are significantly increased by 17.9%, 64.9%, 93.3% and 89.4% as compared to raw Mg, respectively.
In this work, interfacial microstructure in W/2024Al composite and inhibition of the W-Al direct reaction by CeO2 doping were investigated. The composites were prepared through powder sintering, and after preparation the composites were treated by annealing at 823 K. For the prepared W/2024Al composite, a multi-phase thin layer composed of WAl12 and WAl5 compounds were formed at the interface due to the W-Al direct reaction. While doping CeO2 in the composite, Al-Ce-Cu-W amorphous substituting of W-Al compounds were formed at the interfacial reaction layer. In an annealed state, the composite with CeO2 doping shows a significant inhibitory effect on W-Al compounds, which was attributed to the crystallized layer that evolved from Al-Ce-Cu-W amorphous as an interfacial obstacle. The crystallization product for Al-Ce-Cu-W amorphous layer was identified as bcc-structure Al-Ce-Cu-W phase without any binary/ternary Ce-containing phases. Therefore, by doping CeO2 in W/2024Al composite, W-Al direct reaction was markedly inhibited during both preparation and annealing.
Magnesium matrix nanocomposites (MMNC, the same below) containing 2 wt.% nanosized were fabricated through accumulative roll bonding (ARB). The microstructure and mechanical properties of Mg/2 wt.% nanocomposites are reported for various ARB cycles. To evaluate microstructure of the nanocomposites, the field emission scanning electron microscope (FE-SEM), X-ray diffractometer (XRD), and transmission electron microscope (TEM) were applied. After fourteen ARB cycles, the nanocomposite showed a homogeneous distribution of reinforcements and a significant reduction in average matrix grain size. Meanwhile, the nanocomposite revealed a higher percentage of recrystallization and lower intensity of basal texture as compared to monolithic Mg. Mechanical properties were investigated through tensile and microhardness tests. The strength and elastic modulus and microhardness of Mg/2 wt.% were found to be improved significantly from eight ARB cycles and reach maximum values at fourteen ARB cycles. The ultimate tensile strength, yield strength, microhardness, and elastic modulus of Mg/2 wt.% are considerably increased by 17.6%, 61.0%, 72.7%, and 80.8% as compared to raw Mg, respectively.