Mechanical alloying was performed to obtain a composite material with a homogeneous dispersion of silver particles in a poly(vinyl alcohol) (PVA) matrix. Silver is a bactericidal material, and PVA is a widely used biocompatible polymer. Therefore, this mix can lead to a potentially functional biomaterial. This study focuses on the combination of both materials, processed by mechanical alloying, which has a promising application potential. The silver (Ag) used was ultrafine, measuring between 200 and 400 nanometers, produced from silver nitrate (AgNO3) redox. The Attritor high–energy, water–cooled ball mill was used to mill PVA for 4 h, at 600 rpm speed rotation and 38:1 power milling. Mechanical alloying was demonstrated to cause particle refinement in PVA with a timespan of 1 h. A slight additional particle decrease occurred for long–time milling. A milling time of 4 h was used to disperse the silver particles in the polymer matrix homogeneously. Hot pressing films were produced from the obtained dispersion powders. The microstructural features were studied using several material characterization techniques. Antimicrobial Susceptibility Tests (AST), conducted in an in–vitro assay, showed a hydrophilic character of the films and a protection against bacterial growth, making the process a promising path for the production of surface protective polymeric films.
The ultra high molecular weight polyethylene (UHMWPE) shows properties that provide wide industrial and technological interest. To study the influence of iron particles on UHMWPE, the polymer was filled with Fe-powder in different stoichiometries through mechanical alloying (MA). The MA resultant samples were subjected to various analyses aiming at the characterization of mechanical, structural, and hyperfine properties. The tensile test indicated a small change in the stress-strain curves, this change was related to the yield stress. The X-ray diffraction showed the presence of a monoclinic phase, a metastable phase induced by deformation. Mössbauer spectroscopy pointed at the presence of three iron sites: metallic iron, Fe2+ e Fe3+. Considering these results, it is possible to ascertain that the iron weakly changes some properties of the polymer without degradation. There is a clear indication that iron atoms interact with carbon atoms, between the polymer chains, creating cross-links.
Directed Energy Deposition-Laser Beam (DED-LB) is an ideal Additive Manufacturing (AM) process to obtain very complex geometries, which can be important for several applications in industries such as aerospace and biomedical engineering. The present study aims to determine optimized DED-LB parameters for printing 17-7 PH stainless steel, a semi-austenitic precipitation-hardening alloy renowned for its exceptional combination of high yield strength, toughness, and corrosion resistance. The experimental work used different combinations of laser power, scanning speed, and powder feed rate to investigate the effects on the morphology, surface roughness, and microstructure of the deposited material. The results indicated that a powder feed rate of 4.7 g/min yielded uniform beads, reduced surface roughness, and increased substrate dilution, enhancing the metallurgical bond between the bead and substrate. Conversely, higher feed rates, such as a rate of 9.2 g/min, resulted in increased surface irregularities due to an excessive amount of partially melted powder particles. Microstructural analysis, supported by thermodynamic calculations, confirmed a ferritic–austenitic solidification mode. The austenite and ferrite fractions varied significantly, depending mainly on the substrate dilution due to the decrease in aluminum content. The combination of 400 W laser power and a 2000 mm/min scanning speed resulted in the optimal set of parameters, with an approximately 30% dilution and 80% austenite.
1 January 2020 in Brazilian Journal of Development
Caracterização de misturas de peuamm com resíduo de pneu obtidos através de moagem de alta energia / Characterization of blends of peuamm with tire residue obtained by high energy milling