In this work, polymers of poly[(9,9-dioctylfluorenyl-2,7-diyl)-co-triphenylamine] with side chains containing: pyrene (C1), diphenyl (C2), naphthalene (C3), and isopropyl (C6) structures were synthesized via a Suzuki coupling reaction. The structures were verified using NMR and cyclic voltammetry measurements provide the HOMO and LUMO of the polymers. The polymer with pyrene (C1) and naphthalene (C3) produced photoluminescence in the green while the polymer with the side chain containing diphenyl (C2) and isopropyl (C6) produce dual emission peaks of blue-green photoluminescence (PL). In order to examine the electroluminescence properties of the polymers, the solutions were spin-coated onto patterned ITO anode, dried, and subsequently coated with an Al cathode layer to form pristine single layer polymer LEDs. The results are compared to a standard PFO sample. The electroluminescence spectra resemble the PL spectra for C1 and C3. The devices of C2, C3, and C6 exhibit voltage-dependent EL. An additional red emission peak was detected for C2 and C6, resulting in spectra with peaks at 435 nm, 490 nm, and 625 nm. The effects of the side chains on the spectral characteristics of the polymer are discussed.
15 September 2023 in Journal of Engineering Technology and Applied Physics
Poly(3-hexylthiophene) (P3HT) and [6,6]-phenyl-C71 butyric acid methyl ester (PCBM) polymer solar cell is studied by using GPVDM simulations and experiments. The research focuses on the effects of active layer thickness on solar cell structures as bulk heterojunction (BHJ) (ITO/P3HT:PCBM/Al) as compared to a bilayer structure (ITO/P3HT/PCBM/Al). The optimal active layer thickness of 200 nm is obtained in the simulation for BHJ solar structure. The results also indicate that bulk heterojunctions exhibit slightly higher efficiency than bilayer solar cell with the same thickness, possibly due to a better and worthier total surface region for charge separation and reduced recombination between the electrons and holes. BHJ solar cell is fabricated in the experiment by using spin coating. The results show that higher spin speeds result in a thinner active layer, and the device coated at 2500 rpm had the highest power conversion efficiency of 0.91 % because of a higher Isc and fill factor, despite a low absorption. The results suggest that bulk resistance, and morphology of the active layer play important roles in the carrier transport in the P3HT:PCBM solar cell.