James Krzanowski

Prof. James Krzanowski

Mechanical Engineering Department, University of New Hampshire, Kingsbury Hall, 33 Academic Way, Durham, NH 03824, USA

Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
21 July 2014 in Lubricants
Verified
Journal Article
Open access
PDF file
German Fox-RabinovichGerman Fox-Rabinovich
German Fox-Rabinovich
Iosif GershmanIosif Gershman
Iosif Gershman
MHMohamed A. El Hakim
Mohamed A. El Hakim
MSMohamed Shalaby
Mohamed Shalaby
James KrzanowskiJames Krzanowski
James Krzanowski
SVStephen Veldhuis
Stephen Veldhuis
Tribofilms are dynamic structures that form at the interface during frictional sliding. These films play a significant role in friction control, particularly under heavy loaded/high temperature conditions, such as those found at the cutting tool/chip interface. The thermodynamic aspects of tribofilm formation are discussed here. Thermodynamic analysis of entropy production during friction shows that there are two types of tribofilms that affect the wear behavior of a cutting tool: (1) tribofilms forming as a result of the surface modification of the cutting tools with further tribo-oxidation; and (2) tribofilms that form as a result of material transfer from the contacting frictional body (the workpiece) during the tool/chip interaction. Experimental examples are presented, outlining the beneficial role of both types of tribofilms.

30 April 2014 in Coatings
Verified
Journal Article
Open access
PDF file
James KrzanowskiJames Krzanowski
James Krzanowski
DFDaniel J. Foley
Daniel J. Foley
Ti1−xCrxN thin-film samples were sputter-deposited with lateral composition gradients x = 0.1–0.9 across each sample. In order to determine the effect of Cr content on oxidation, samples were air-oxidized at temperatures ranging from 650 to 950 °C. The extent and type of oxide formed was characterized using X-ray diffraction. Only minor oxidation was observed for the 650–750 °C temperature range. At 850 °C, films below x = 0.7 showed poor oxidation resistance, with the formation of TiO2 and Cr2O3 oxides, but little oxidation occurred above x = 0.7. At 950 °C, films above x = 0.7 again exhibited the best oxidation resistance. Chromium nitride films, which deposited as Cr2N, were found to begin oxidizing at 750 °C, indicating that the increased oxidation resistance of the higher-Cr Ti-Cr-N films can be attributed to the Ti-induced stabilization of the B1-structured phase. A compositionally-uniform film (x = 0.79) was also deposited and analyzed by XPS before and after oxidation. Oxidation resulted in primarily Cr2O3 at the surface, with some TiO2 also present, with the oxide richer in Cr than the starting film composition. These results suggested that at higher Cr compositions in the film, the oxidation mechanism was controlled by Cr diffusion to the surface.

15 October 2020 in Coatings
Verified
Journal Article
Open access
PDF file
FAFaisal Alresheedi
Faisal Alresheedi
James KrzanowskiJames Krzanowski
James Krzanowski
An X-ray diffraction investigation was carried out on nitrogen-containing 304 stainless steel thin films deposited by reactive rf magnetron sputtering over a range of substrate temperature and bias levels. The resulting films contained between ~28 and 32 at.% nitrogen. X-ray analysis was carried out using both the standard Bragg-Brentano method as well as area-detector diffractometry analysis. The extent of the diffraction anomaly ((002) peak shift) was determined using a calculated parameter, denoted RB, which is based on the (111) and (002) peak positions. The normal value for RB for FCC-based structures is 0.75 but increases as the (002) peak is anomalously displaced closer to the (111) peak. In this study, the RB values for the deposited films were found to increase with substrate bias but decrease with substrate temperature (but still always >0.75). Using area detector diffractometry, we were able to measure d111/d002 values for similarly oriented grains within the films, and using these values calculate c/a ratios based on a tetragonal-structure model. These results allowed prediction of the (002)/(200) peak split for tetragonal structures. Despite predicting a reasonably accessible split (~0.6°–2.9°–2θ), no peak splitting observed, negating the tetragonal-structure hypothesis. Based on the effects of film bias/temperature on RB values, a defect-based hypothesis is more viable as an explanation for the diffraction anomaly.