Yttrium oxide (Y2O3) and yttrium oxyfluoride (YO0.6F2.1) protective coatings were prepared by an atmospheric plasma spraying technique. The coatings were exposed to a NF3 plasma. After the NF3 plasma treatment, the mass loss of the coatings showed that the etching rate of YO0.6F2.1 was larger than that of the Y2O3. X-ray photoelectron spectroscopy revealed that YO0.5F1.9 was present in the Y2O3 coating, whereas YO0.4F2.2 was present in the YO0.6F2.1 coating. Transmission electron microscope analysis conducted on contamination particles generated during the plasma etching showed that both coatings were mainly composed of YFx. The contamination particles estimated by in-situ particle monitoring sensor revealed that the YO0.6F2.1 compared with the Y2O3 coatings produced 65% fewer contamination particles.
The internal coatings of chambers exposed to plasma over a long period of time are subject to chemical and physical damage. Contamination particles that are produced by plasma damage to coatings are a major contribution to poor process reliability. In this study, we investigated the behavior of contamination particles produced from plasma damage to Y2O3 and YF3 protective coatings, which were applied by an aerosol deposition method. The coating materials were located at the powered electrode, the grounded electrode, and the grounded wall, which were exposed to a NF3 plasma. The mass loss at the powered electrode, which was exposed to the NF3 plasma etching under an applied bias, showed that the YF3 etching rate was higher than that of Y2O3. Conversely, the mass of coating increased at the grounded electrode and the grounded wall, which were exposed to NF3 plasma etching under zero bias. The mass of the Y2O3 coating increased more than that of the YF3 coating. X-ray photoelectron spectroscopy analysis showed that the Y2O3 coating corroded to YOxFy in the NF3 plasma, and YF3 existed as YFx. Light scattering sensor analysis showed that the YF3 coating produced fewer contamination particles than did the Y2O3 coating.
The effect of growth temperature on the atomic layer deposition of zirconium oxide (ZrO2) dielectric thin films that were fabricated using a CpZr[N(CH3)2]3/C7H8 cocktail precursor with ozone was investigated. The chemical, structural, and electrical properties of ZrO2 films grown at temperatures from 250 to 350 °C were characterized. Stoichiometric ZrO2 films formed at 250–350 °C with an atomic ratio of O to Zr of 1.8–1.9 and a low content of carbon impurities. The film formed at 300 °C was predominantly the tetragonal crystalline phase, whereas that formed at 350 °C was a mixture of tetragonal and monoclinic phases. Electrical properties, such as capacitance, leakage current, and voltage linearity of TiN/ZrO2/TiN capacitors fabricated using the thin ZrO2 films grown at different temperatures were compared capacitor applications. The ZrO2 film grown at 300 °C exhibited low impurity content, predominantly tetragonal crystalline structure, a high dielectric permittivity of 38.3, a low leakage current of below 10−7 A/cm2 at 2 V, and low-voltage linearity.
The parts of equipment in a process chamber for semiconductors are protected with an anodic aluminum-oxide (AAO) film to prevent plasma corrosion. We added cerium(IV) ions to sulfuric acid in the anodizing of an AAO film to improve the plasma corrosion resistance, and confirmed that the AAO film thickness increased by up to ~20% when using 3 mM cerium(IV) ions compared with general anodizing. The α-Al2O3 phase increased with increasing cerium(IV) ion concentration. The breakdown voltage and etching rate improved to ~35% and 40%, respectively. The film’s performance regarding the generation of contamination particles reduced by ~50%.