The mechanical properties of single Yushania alpina bamboo fibers have not been explored. This is a serious limitation on their application. The main purpose of this work is to fill up information gaps to prepare for the growing usage of Ethiopian bamboo in a variety of applications. This study looks at the characterization and optimization of Y.alpina bamboo fiber properties extracted both chemically and mechanically. Using response surface methodology (RSM) the mechanical properties were optimized and linear, quadratic and interaction of independent variables were determined. Samples of length 25–30 cm were harvested at various ages from the middle of the stem which was then soaked in different NaOH concentrations weight by volume for different times. Using a rolling machine that has three rollers, the fiber is mechanically extracted. The optimal mechanical properties were observed at plant age of 1.8 years, alkali concentration of 10%, and a soaking duration of 2.0 days. The model is significant (P ≤ 0.005) with a 95% confidence level for predicted values that were closer to the measured values, indicating that the model's fit to the measured properties was strong at the optimized values. The optimized points of age and soaking duration ware subjected to chemical, thermal and morphological analysis for each corresponding NaOH Concentration (6, 12, and 18%) levels. Scanning electron microscopy (SEM) was employed to examine the microstructure of the fibers and discovered that the 18% NaOH treated fiber resulted in more wrinkles in the surface of bamboo fibers when compared with the 6 and 12%NaOH Bamboo fiber. Using thermogravimetric analysis (TGA) and differential thermal gravimetric (DTG), the study investigated weight loss increased as alkali concentration increased but the scenario functioned for proper concentration.
21 May 2024 in Case Studies in Thermal Engineering
The primary energy source in Ethiopia is biomass. Over 80 of Ethiopians are rural dwellers who rely on biomass energy for lighting and cooking. In most parts of Ethiopia, injera is traditionally baked using an open fire, a three stone, or a device using woody biomass. These baking stoves have very low efficiency and consume a significant amount of fuel. Moreover, these traditional baking stoves have released large amounts of indoor air pollution, which has led to different types of health-related risks, especially for women and children in the country. Therefore, the aim of this study was to investigate efficient and fuel-saving injera baking technologies. Rigorously, an injera baking gasifier stove was designed, developed, and characterized in detail through water boiling and control cooking test methods. The indoor air pollution level was evaluated using particulate matter measuring instruments. The result indicated that the developed gasifier stove had a thermal efficiency of 21.8. Furthermore, an 86 fuel savings performance was demonstrated by the controlled cooking test for the injera baking gasifier stove. The average emission concentrations of particulate matter and carbon monoxide were 608µg/m3 and 9ppm, respectively, during indoor air pollution determination. The study showed that injera baking gasifier stoves are a promising cooking technology for societies where baking is mostly dependent on traditional biomass fuel.
In this experimental study, untreated Ethiopian high land bamboo fibres were characterized and detected the optimal properties. In the investigation, SEM was applied to examine the surface texture of the fibres. The chemical bonds of the molecules (functional groups) were identified by Fourier transform infrared spectra (FTIR). The thermal properties of the fibre were explored with a thermogravimetric analyser, and the results were confirmed by differential thermo-gravimetric analysis (DTG). Mechanical properties were improved using the experimental design principle. The design is based on the RSM methodology three-factor three-level to present mathematical models. At various plant ages, the culm wall thickness in the radial direction and soaking duration of the single fibre is extracted using a roller crusher machine. The operating parameters and optimal mechanical properties were validated using confirmation tests. Breaking force 796.5cN, tenacity 46.8cNtex-1, work done 456cNmm, and modulus 1814cNtex-1 were the optimal mechanical characteristics achieved at the operating parameters 2.0 years age, a calm thickness layer coded values of 0.6 along the radial direction, and 3.8 days soaking time when compared to mechanical properties 1–3 years plant age, calm thickness layers of from primary (-1) to secondary layers (1) along with the radial direction, and 3–9 days soaking time.
10 November 2022 in International Journal of Polymer Science
Characterization of thermal properties of different ages highland bamboo fiber attributes extracted chemically and mechanically is the focus of this study. Samples of length 2530cm were harvested at various ages from the middle of the stem, which was then soaked in different NaOH weight-by-volume concentrations and soaked in water for different days. Using a rolling machine that has three rollers, the fiber is mechanically extracted. The sample was subjected to different analyses for each corresponding age (1, 2, and 3 years) and NaOH concentration (untreated, 1, 2, and 3) levels using thermogravimetric analysis, differential scanning calorimetry, derivative thermogravimetric analysis, and differential thermal analysis for thermal property characterization. Scanning electron microscopy (SEM) was used for morphological studies, whereas Fourier transform infrared spectroscopy (FTIR) was used for the identification of functional groups of the fibers. The surface appearance of the cell wall and microfibril aggregates were changed by alkali treatment. From the SEM results, 3 NaOH-treated fiber resulted in more wrinkles on the surface of bamboo fibers when compared with the 1 and 2 NaOH bamboo fibers. Using thermal analysis measurements, this study investigated that weight loss increased as alkali concentration increased, but the scenario functioned for proper concentration. The first degradation stage is responsible for the biggest weight loss since it includes the disintegration of all of the fibers primary components (cellulose, hemicellulose, and lignin).
6 December 2024 in Environmental Progress & Sustainable Energy